PRODUCT NO. Manufacturer Trade Name
RTP Company RTP 1381  Polyphenylene Sulfide (PPS) Carbon Fiber 10%  (discontinued **)
RTP Company RTP 1381 C  Polyphenylene Sulfide (PPS) Carbon Fiber 10%  (discontinued **)
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5 BK PPS, linear, with carbon fiber and PTFE Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301/CF/20 PPS, linear, with carbon fiber Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301/XCF/30 N PPS, linear, with carbon fiber Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-7449 PPS, linear, with carbon fiber and PTFE Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-7815 PPS, linear, with carbon fiber, lubricant modified Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-7953 PPS, linear, with carbon fiber and PTFE Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-8066 PPS, linear, with carbon fiber, lubricant modified, high viscosity Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-8077 PPS, linear, with carbon fiber Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-8306 PPS, linear, with carbon fiber, lubricant modified Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-8367 PPS, linear, with CNT Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-8400 PPS, linear, with carbon fiber, PTFE, lubricant modified Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-8457 PPS, linear, with carbon fiber, lubricant modified Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-8517 PPS, linear, with carbon fiber Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-0825 PPS, linear, with carbon fiber Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-0915 PPS, linear, with carbon fiber, PTFE, lubricant modified Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-7629/EG PPS, linear, with carbon fiber Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-7767 PPS, linear, with carbon fiber, lubricant modified Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-7896 PPS, linear, with carbon fiber, thermally conductive modified Lehmann & Voss & Co. LUVOCOM®
Techmer ES Electrablend® PPS 05002 Techmer ES Electrablend®
Techmer ES Electrablend® PPS 06001 Techmer ES Electrablend®
RTP Company RTP 1381 C AR 12 Polyphenylene Sulfide (PPS), Carbon Fiber - Aramid Fiber RTP Company
RTP Company RTP 1381 C TFE 15 Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced - PTFE Lubricated RTP Company
RTP Company RTP 1381 D TFE 13 SI 2 Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced - PTFE & Silicone Lubricated RTP Company
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-0824 PPS, linear, with carbon fiber Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5-1 PPS, linear, with carbon fiber and PTFE Lehmann & Voss & Co. LUVOCOM®
Lehmann & Voss LUVOCOM® 1301-7804 PPS, linear, with carbon fiber, thermally conductive modified Lehmann & Voss & Co. LUVOCOM®