Physical Properties Metric English Comments
Density >= 0.0240 g/cc
>= 0.000868 lb/in³
Single Pass Continuous Expansion
NOVA Chemicals EPS M97BC Low Volatile/Low Pentane Modified Expandable Polystyrene
Applications: Insulation, SIP's, ICF's, fabricated packagingInformation provided by NOVA Chemicals.
Density >= 0.0240 g/cc
>= 0.000868 lb/in³
Single Pass Continuous Expansion
NOVA Chemicals EPS M97C Expandable Polystyrene Resin
Applications Insulation, SIP's, ICF's, Fabricated PackagingInformation provided by NOVA Chemicals
Density 0.0240 - 0.0400 g/cc
0.000867 - 0.00145 lb/in³
molding density range
IRPC Polimaxx Pentfoam 455E Expandable Polystyrene
GENERAL: PENTFOAM "455E" IS A SELF EXTINGUISHING (SE) GRADE EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST CYCLES IN VACUUM MOL..
Density 0.0240 g/cc
0.000868 lb/in³
Unifrax Fiberfrax® Fibermax® Mat Ceramic Fiber Insulator
Fibermax Mat is a high-temperature, flexible mat product that is lightweight (1.5 lb/ft3 density) and highly resilient. It is composed entirely of Fibermax polycrystalline mullite fibers to produce..
Density 0.0240 g/cc
0.000867 lb/in³
Nominal skin/skin; BS ISO 7214 1998
Zotefoams Plastazote® LD24FM Low Density Polyethylene Foam, Flame Retarded
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0240 g/cc
0.000867 lb/in³
Nominal skin/skin; BS ISO 7214 1998
Zotefoams Plastazote® LD24FR Low Density Polyethylene Foam, Flame Retardant
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0240 g/cc
0.000867 lb/in³
Nominal skin/skin; BS ISO 7214 1998
Zotefoams Plastazote® LD24LC Low Density Polyethylene Foam, Large Cell
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0240 g/cc
0.000867 lb/in³
Nominal skin/skin; BS ISO 7214 1998
Zotefoams Plastazote® LD24MC Low Density Polyethylene Foam, Medium Cell
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0240 g/cc
0.000868 lb/in³
Hexcel® HexWeb® HRH-10 - 1/4 - 1.5 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Density 0.0240 g/cc
0.000868 lb/in³
Hexcel® HexWeb® HRH-10 - 3/16 - 1.5 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Density 0.0240 g/cc
0.000868 lb/in³
Hexcel® HexWeb® HRH-10 - 3/4 - 1.5 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Density 0.0240 g/cc
0.000868 lb/in³
Hexcel® HexWeb® HRH-78 - 3/8 - 1.5 Commercial Grade Nomex Honeycomb/Phenolic Resin
Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after..
Density 0.0240 g/cc
0.000868 lb/in³
Hexcel® HexWeb® HRH-10 - 3/8 - 1.5 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Density 0.0240 g/cc
0.000867 lb/in³
Nominal skin/skin; BS ISO 7214 1998
Zotefoams Plastazote® LD24 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0240 g/cc
0.000867 lb/in³
Nominal skin/skin; BS ISO 7214 1998
Zotefoams Plastazote® MP24 Metallocene Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0240 - 0.0270 g/cc
0.000867 - 0.000975 lb/in³
Akzo Nobel Expancel® 091 WE 40 d24 Wet expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density 0.0240 g/cc
0.000868 lb/in³
Free Rise Density, 4% H<sub>2</sub>O
ACC EP LS EPI Engineered Polymers Leak Stop MDI
EP LS, “Powered by Reactamine® Technology”, is a special MDI prepolymer designed to be pumped into voids or walls. EP LS reacts with water to create a shaving cream-like foam. This foam will soli..
Density 0.0240 - 0.0400 g/cc
0.000867 - 0.00145 lb/in³
molding density range
IRPC Polimaxx Pentfoam 328H Expandable Polystyrene
General: Pentfoam 328H is a high density grade expandable polystyrene containing pentane as blowing agent, this grade is developed to meet the demand for fast molding cycles in vacuum machineApplica..