Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.914 - 0.918 g/cc | 0.0330 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4115N (16401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.914 - 0.918 g/cc | 0.0330 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4116N (16401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
Huntsman Rexell® V8801 Cast Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ExxonMobil Method |
ExxonMobil LD 509.48 Compounding Resin
(discontinued **) LD 509.48 is a high melt index homopolymer resin designed to provide good processability in compounding applications.Information provided by ExxonMobil Chemical |
|||
Density | 0.914 - 0.918 g/cc | 0.0330 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4115P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.914 - 0.980 g/cc | 0.0330 - 0.0354 lb/in³ | Average value: 0.945 g/cc Grade Count:71 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | Yield Density |
Honeywell PMP Polymethylpentene Film
(discontinued **) PMP is a clear, red, or blue film manufactured from polymethylpentene. It provides more toughness and heat resistance than standard polyolefins for release film applications.Information provided by.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5051 800 Micron LDPE Powder Description: ICOFLO 510-5051 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5058 1200 Micron LDPE Powder Description: ICOFLO 510-5058 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5062 500 Micron LDPE Powder Description: ICOFLO 510-5062 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOTEXâ„¢ 520-5050 500 Micron LDPE Powder Description: ICOTEX 520-5050 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and fa.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5064 1200 Micron LDPE Powder Description: ICOFLO 510-5064 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc @Temperature 121 °C |
0.0330 lb/in³ @Temperature 250 °F |
Dry Density |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M44 Moldable Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or .. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
UBE UMERIT 1520F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® D163 Metallocene Linear Low Density Polyethylene, Blown Film This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 650 Low Density Polyethylene Resin (European Grade) Product Description: LD 650 is an easy flowing LDPE grade with a good flexibility and excellent toughness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 654 Low Density Polyethylene Resin (European Grade) Product Description: LD 654 is a very high flow LDPE grade with a very good flexibility. It can be added to low-flowing LDPE grades to improve their processability.Availability: Africa & Middle East.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 655 Low Density Polyethylene Resin (European Grade) Product Description: LD 655 is a very high flow LDPE grade with a very good flexibility. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabiliz.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | |
Dow AFFINITY™ SM 1350 Polyolefin Plastomer AFFINITY® SM 1350 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in durable injection molded housewares and compression molded closure liners or gaskets. It exhibit.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | |
Dow ATTANE™ 4301 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4301 copolymer is an ultra low density polyethylene having high impact resistance and tear strength in blown films, designed for use in food packaging applications. It has low levels of sli.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | |
Dow ATTANE™ 4501 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4501 copolymer is an ultra low density polyethylene having high tear strength and impact resistance, designed for use in industrial/ consumer film applications, either as a high performance.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | |
Dow ATTANE™ 4701 Ultra Low Density Polyethylene, Medical Packaging Grade ATTANE® 4701 copolymer is an ultra low density polyethylene having high pinhole and puncture resistance, tear strength and high impact resistance combined with improved softness. It has low levels .. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM C134 |
BNZ Materials BNZ-26 HS Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Density | 0.914 g/cc @Temperature 23.0 °C |
0.0330 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Arkema Group OREVAC® 18360 Maleic Anhydride Modified Polyethylene OREVAC® 18360 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | |
BASF N-Ethylethanolamine Formula: C4H11NOCAS: 110-73-6Description: N-Ethylethanolamine is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: EEA, 2-Ethylaminoethanol, 2-(Ethylamino)etha.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | ASTM D1505 |
Huntsman Rexell® V8403 Cast Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and.. |
|||
Density | 0.914 g/cc | 0.0330 lb/in³ | |
ConocoPhillips 32 Spectrum Cutting Oil Description: Conoco Spectrum Cutting Oil is a multifunctional cutting fluid formulated with a sulfurized base oil, is a balanced additive system and is suited for a wide variety of machining applica.. |