Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.922 - 0.924 g/cc | 0.0333 - 0.0334 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® CX 7020 LDPE - Cast Film The Trithene® CX 7020 resin is a low-density polyethylene (LDPE) with medium molecular weight, excellent processability, and low gel content. Those features allow a production of thin and highly un.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
SABIC HP4023W Low Density Polyethylene for Blown Film Product Description: HP4023W is a Low Density Polyethylene grade suitable for producing general purpose films and contains slip and antiblock additives. It yields excellent processability with goo.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® L42108E2 Film (Butene Grade) LLDPE
(discontinued **) Butene Copolymer (High slip and antiblock)Applications: Thin gauge blown film with improved stiffnessThin gauge blown film with improved stiffnessInformation provided by Formosa Plastics Corporation.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D 4883 |
Eastman 1810A Polyethylene
(discontinued **) Polyethylene 1810A contains no additives. It is suggested for injection molding applications.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to West.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 1.25 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Huntsman PE1068 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Exceptional draw down and processability even to 1/2 mil; excellent strength, good heat sealability, and good optical.FDA Notes: Conforms to FDA regulation 21.. |
|||
Density | 0.921 - 0.970 g/cc | 0.0333 - 0.0350 lb/in³ | Average value: 0.931 g/cc Grade Count:191 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Density | 0.922 - 0.925 g/cc | 0.0333 - 0.0334 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TS 7045 LDPE - Film - Plastification The Trithene TS 7045 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |
|||
Density | 0.922 - 0.924 g/cc | 0.0333 - 0.0334 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TX 8024 LDPE - High Clarity Film The Trithene TX 8024 resin is a low-density polyethylene (LDPE) with high molecular weight and distribution narrow, designed to obtain films with very high clarity and excellent processability. This.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1475 |
Humiseal 1B73 Acrylic Conformal Coating Humiseal 1B73 Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityUL ApprovedMIL-I-46058C ApprovedPasses thermal sho.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® NA345184 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | GOST 15139 |
Sibur 15303-003 Low Density Polyethylene For production of films and film articles, including thermoset films, thin films, food contact grade films
(including tight packing), general-purpose films, and bags. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | base resin; ISO 1183/ISO 1872-2 |
Borealis Superclean™ LE4201EHV Polyethylene Insulation Compound, Crosslinkable Superclean™ LE4201EHV is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: Superclean™ LE4201EHV is intended for insulation of XLPE extr.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | base resin; ISO 1183/ISO 1872-2 |
Borealis Superclean™ LE4244S Polyethylene Insulation Compound, Crosslinkable Superclean™ LE4244S is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: Superclean™ LE4244S is intended for insulation of XLPE High Vol.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 5619 LDPE Shrink and Heavy Duty Packaging Film Resin Resin Type: HomopolymerCharacteristics: Excellent Tensile and Impact Strength, Good Abrasion and Tear Resistance, Good Resistance to Blocking, Wide Range of Shrinkage Characteristics, Low Slip, Low .. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® HHM TR 257 LLDPE Blown Film Resin Resin Type: Medium molecular weight distributionCharacteristics: Combination of toughness and tensileGood puncture resistanceMeets FDA regulations for food packaging below cooking temperaturesInform.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 1107X95 Linear Low Density Polyethylene Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | |
Dow LDPE 135A Low Density Polyethylene, Blown Film Grade DOW LDPE 135A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of slip .. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
Dow LDPE 586A Low Density Polyethylene, Packaging Grade DOW LDPE 586A resin is used for general purpose packaging applications. It contains medium levels of slip additive and low levels of antiblock additive. This material complies with U.S.FDA regulatio.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
Dow LDPE 641I Low Density Polyethylene, Liner Film Grade DOW LDPE 641I resin is a general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. It contains medium levels of slip additive and low levels of an.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | |
Dow LDPE 955I Low Density Polyethylene DOW LDPE 955I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility, and good toughness, with low warpage. Typical applications include lid.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | |
Dow LDPE 5004I Low Density Polyethylene, Extrusion Coating Grade DOW Polyethylene 5004I extrusion coating resin is a low melt index resin for heavy duty applications such as paperboard coatings, milk cartons and folding cartons, aseptic package coatings, bag line.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM-D792 |
Braskem LL6800N LLDPE Blown Film Extrusion Polyethylene Copolymer LL6800N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains antiblock, proc.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D-1505 |
Bapolene® 213B Polyethylene, Extrusion Grade Bapolene 213B is a low density polyethylene for molding, extrusion and foaming applications. It contains slip and complies with US FDA regulation 21 CFR 177.1520 (Olefin polymers), paragraph (c)2.1.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM-D1505 |
Braskem EG0921 LDPE Blow Molding Polyethylene EG0921 is a low-density polyethylene with good mechanical properties and environmental stress cracking resistance (ESCR) and excellent sealability. It is used in blow molded parts and medium-resista.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ExxonMobil Method |
ExxonMobil LD 419.MV Wire & Cable Resin
(discontinued **) LD 419.MV is a LDPE designed for wire and cable applications and is suitable for making crosslinkable compounds for medium voltage insulation.Information provided by ExxonMobil Chemical |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Huntsman PE2065 Injection Molding Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: General purpose injection molding resin with good flow characteristicsApplications: Injection molding: lids.FDA Notes: Conforms to FDA regulation 21 CFR 177.1.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Huntsman PE6010 Blow Molding Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, complies with USP Classification VI, and FDA compliant.Features: Meets exacting requirements of blow molded containers and processes well with parison s.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 11E1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, strength and toughness.Applications: Base resin.Data provided by the manufacturer. |