Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® TF-0338-E Hexene LMDPE Film Resin Excellent stiffness and glossApplications: Diaper back sheet, BlendingAdditives: High temperature AOFilm properties are typical of film extruded at 280°C.Information provided by NOVA Chemicals. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® TI-0338-A MDPE Masterbatch Resin Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | Exxon Method |
ExxonMobil Optema® TC-113 Ethylene Methyl Acrylate for Compounding
(discontinued **) Data provided by the manufacturer, Exxon Chemical.23.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used as an impact modifier or compatibilizer in polymer compounds. It ca.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D4883 |
ExxonMobil LL 8401.67 Rotational Molding Resin
(discontinued **) LL 8401 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for Non-UV applications that require optimum balance of flow processabil.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D4883 |
ExxonMobil LL 8450 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. This resin is ideally suited for applications that require optimum balance.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9301 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234360A; ASTM D 4976 Classification: PE 225, A 56607Applications:Base Resin for use in Gas, Oil Patch and Industrial Pipe.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9638 HDPE Sheeting and Blown Film Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Cast Geomembrane Applications, Notion and Millinery Bags, Heavy Duty Shipping Sacks, In.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9642 HDPE Sheeting Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Blown Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Contain.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Eastman 5223 LDPE 6% VA Copolymer, High Clarity, Ultra-High Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent impact strength, Good heat seal characteristics, High antiblock, No Slip, Good processability. Slip 0 ppm. Antiblock 5000 ppm.Applications:Ice ba.. |
|||
Density | 0.938 - 1.01 g/cc | 0.0339 - 0.0365 lb/in³ | Average value: 0.954 g/cc Grade Count:266 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Density | 0.937 - 1.06 g/cc | 0.0339 - 0.0383 lb/in³ | Average value: 0.957 g/cc Grade Count:19 |
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is .. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | Natural; ASTM D4883 |
Ineos TUB 172 HDPE TUB 172 is a yellow medium density polyethylene copolymer designed specifically for the extrusion of natural gas pipe. It exhibits excellent long term stress life and slow crack growth resistance. T.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D792 |
Lushan L-5R (HC) Polyethylene Copolymer Adhesive for Steel Pipe Coating Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and pro.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) MF3820 High Density Polyethylene MF-3820 is a high molecular weight high density polyethylene. Application: bottle extrusion.Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® HHM TR-130 MDPE Film Resin Medium density resin provides overall balance of tensile, impact, and tear properties in film. It is suited for merchandise, produce, and trash bags. Processing performance is excellent on high st.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® K306 Fully Formulated Medium Density Hexene Copolymer Fully Formulated Medium Density Hexene CopolymerCustomer Benefits: This extrusion grade hexene copolymer has good processability, excellent melt strength, broad fusion range, outstanding ESCR, meets.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | Base Density; ASTM D1505 |
Chevron Phillips Marlex® M358Y3 LLDPE Pipe and Corrugated Extrusion Resin Characteristics: High visibility as gas pipingGood outdoor storage length when blended with natural MDPE containing UV stabilizerGood long-term hoop strengthApplications: PipesNot recommended for co.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 15019CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 15019CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applications: Hot.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Appeel® 22D843 Ethylene Acrylate DuPont™ Appeel® 22D843 is a polypropylene modified ethylene acrylate resin designed to function as a masterbatch to achieve peelability in polypropylene based sealant layers. It provides peelable .. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Fusabond® E589 Polymer Modifier DuPont™ Fusabond® E589 is an anhydride modified polyethylene. Uses: Adhesives Pipe Coating Tie-Layer Features premium adhesive for Pipe Coating tie-layer at high surface temperatures. ( 90°C) |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | natural resin; ASTM D792 |
Dow DFDC-7525 NT High Density Polyethylene Resin DOW DFDC-7525 NT is produced using UNIPOL™ process technology. It is intended for use in thin wall drip tape and micro-irrigation tube, hose and tube, and profile extrusion applications. Informati.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | |
Dow Primacor® 3460 Ethylene Acrylic Acid (EAA) PRIMACOR® 3460 polymer containing 9.5% comonomer is a heat seal coating for high speed packaging applications where low temperature processing is necessary for minimal taste and odor effects. It is.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Bapolene® 3039U Polyethylene, Rotational Molding Grade Bapolene 3039U is a hexene linear low density polyethylene designed to provide superior impact resistance. It contains a UV-stabilization package and complies with US FDA 21CFR177.1520.Applications.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Arkema Group OREVAC® 9307 Y EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 8306 BK, 8306G BK MDPE Rotational Molding Resin
(discontinued **) Features: Balanced combination of toughness, ESCR and processability.Applications: General purpose.Data provided by the manufacturer. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® TR-0338-UG MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ISO 1183 |
Borealis Borstar® FB4370 Medium Density Polyethylene Borstar® FB4370 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Applications: Borstar® FB4370 has been developed especially for ap.. |