Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 58G (High Gloss) HDPE Blow Molding Resin
(discontinued **) Features: Outstanding gloss, pearlescent finish when colored, good processability.Applications: Small part blow molding, injection blow molding, low-moderate ESCR uses.Data provided by the manufactu.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D4883 |
ExxonMobil HD 9856BA Blow Molding Resin
(discontinued **) HD 9856BA is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856BA exhibit a unique combination of stiffness and environmental stress cracki.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D 792 |
NOVA Chemicals Sclair® 2906 HDPE Injection Molding Resin NOVA Chemicals' polyethylene resins are chemically and biologically inert.Features: Excellent toughness and impact resistance, High stiffness, Excellent processing stability, High GlossAdditives: .. |
|||
Density | 0.958 - 0.964 g/cc | 0.0346 - 0.0348 lb/in³ | |
Kazanorgsintez 294-73 High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: Composition of HD grad.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D1475 |
Humiseal 1A27 Urethane Conformal Coating Humiseal 1A27 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedPasses thermal shock test (MIL-I-46058C)Flammabilit.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D1475 |
Humiseal 1B73LSE Acrylic Conformal Coating Humiseal 1B73LSE Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityUL Approval PendingMIL-I-46058C Approval Pendin.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D1475 |
Humiseal 1C65 Silicone Conformal Coating Humiseal 1C65 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® M6028 High Density Polyethylene ApplicationsM 6028 is a homopolymer that is warp resistant, exhibits excellent toughness, stiffness and color as well as low odor and good processing stability. Typical applications include safety .. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Black; ASTM D4883 |
Ineos TUB 121 HDPE TUB 121 (aka ELTEX® TUB 121, ELTEX® TUB 121 N2025, and ELTEX® TUB 121 N3000) is a black high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, ind.. |
|||
Density | 0.958 - 0.964 g/cc | 0.0346 - 0.0348 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GF 4960 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.959 - 1.01 g/cc | 0.0346 - 0.0364 lb/in³ | |
Lord Adhesives 551 Very Low Viscosity, Adhesive Thinner, Medium Cure Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ASTM D1505 |
Iran Petrochemical (PCC) HB0035 High Density Polyethylene HB0035 is a high molecular weight high density polyethylene blow molding grade combining blow molding extrusion behavior and superior mechanical properties. Blow molded items made from HB 0035 exhi.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D792 |
IRPC Polimaxx Polene R1760 High Density Polyethylene CHARACTERISTICS: HIGH IMPACT STRENGTH, EXCELLENT SURFACE APPEARANCE, GOOD RIGIDITY CONTAIN UV STABILIZER ADDITIVEAPPLICATIONS: INJECTION MOLDING FOR CRATES, TRAYS, CASES, INDUSTRIAL PARTS, BINS, LAR.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA556 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Information provided by Illinois Tool Works.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D792 |
LyondellBasell Alathon® L5885 High Density Polyethylene ApplicationsALATHON L 5885 is a medium molecular weight high density homopolymer for use in blown film applications. Typical applications include those low WVTR requirements.Regulatory StatusL 5855.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D1505 |
Iran Petrochemical (PCC) 60507 High Density Polyethylene 60507 is a HDPE injection molding grade which combines good flowability with balanced physical properties. This resin is well suited for general purpose applications requiring high stiffness. Applic.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) I3 HC 7260(THE) High Density Polyethylene I3 (HC 7260) is a high density polyethylene with propylene as comonomer. The product has good impact strength, good stress cracking resistance, low warping and good flow ability as well as high dens.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) I3S HC 7260(THE) High Density Polyethylene I3 is a high density polyethylene with 1-Butene as co monomer. It has low warpage, good flowability, high density, hardness and stiffness, good impact strength, and good stress cracking resistance... |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Compound; ISO 1183 |
Borealis BorPEX™ HE2558 Blue High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide)) BorPEX HE2558 is a blue, high molecular weight, high density polyethylene compound for crosslinkable pipes, specially designed for peroxide crosslinking. Long stability and UV resistance is ensured.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ISO 1872-2/ISO 1183 |
Borealis BorSafe™ HE3494-LS-H HDPE Compound for Pressure Pipes BorSafe™ HE3494-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ISO 1183 |
Borealis FL5580 High Density Polyethylene FL5580 is a high density polyethylene with an excellent combination of extrusion properties and moisture barrier properties. Applications: FL5580 has been developed especially for applications like.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | ISO 1872-2/ISO 1183 |
Borealis BorSafe™ HE3490-IM HDPE Compound for Injection Molded Pressure Fittings BorSafe™ HE3490-IM is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by .. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D792 |
CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene Hitec pipe grade HDPE is a special formulation that has high impact strength, and environmental stress crack resistance. Hitec Pipe grade meets Federal specification L-P 390C, ASTM D1248 Type III we.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | |
Dow Primacor® 5980I Ethylene Acrylic Acid (EAA) PRIMACOR® 5980I dispersible polymer is an ethylene acrylic acid copolymer (20 wt % comonomer) which is dispersible in aqueous alkali and amines. Excellent adhesion to metallic, cellulosic, glass an.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Part B |
Abatron SS-Bond-P™ Stainless-Steel-Filled, Structural Adhesive Putty; Paste SS-Bond-P™ is a stainless-steel-filled structural adhesive putty. Used where a filler is needed that is as heavy, hard, and wear resistant as iron, but rustproof and more chemical resistant. Common.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM-D792 |
Braskem IB58 HDPE Injection Molding Polyethylene Copolymer IB58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers good processability combined with good .. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | Part B |
Abatron BronzeWeld-P™ Bronze-Filled, Structural Adhesive Putty; Paste BronzeWeld-P™ is a bronze-filled structural adhesive putty. Ideal for statuary, antiques, boats, transportation equipment, vases, railings, metal furniture, metal trim, frames, and instruments. Use.. |
|||
Density | 0.959 g/cc | 0.0346 lb/in³ | AboCure 50-4 |
Abatron AboCast 50-11/AboCure 50-4 Epoxy AboCast 50-11 is a clear unfilled resin with low viscosity and a weight of 9.5 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. A.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | Exxon Method |
ExxonMobil Escorene® HDZ-128 MMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.Can be processed on high stalk, pocket extrusion or cast lines. Films made from HDZ-128 exhibit an excellent stiffness balance. High thermal stabi.. |
|||
Density | 0.957 g/cc | 0.0346 lb/in³ | ASTM D792-ISO 1183 |
DuPont Elvax® 150W-LG Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 150W-LG is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent th.. |