Polymer Property : Density = 0.0353 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.978 g/cc
0.0353 lb/in³
NEU NeuSoft™ 597-50A Industrial Ether TPU / SBC blend
Density 0.978 g/cc
0.0353 lb/in³
ASTM D792
North Wood Plastics 60 PP + UNIFILL (20% Wood Fiber)
Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It..
Density 0.978 g/cc

@Temperature 20.0 °C
0.0353 lb/in³

@Temperature 68.0 °F
LyondellBasell Glycol Ether DBA Diethylene glycol butyl ether acetate
Information provided by Lyondell.
Density 0.977 - 1.013 g/cc
0.0353 - 0.03660 lb/in³
Lord Adhesives Flocklok® 853 Blocked Flock Adhesive
Flocklok® 853 is a blocked, heat-curing, single coat adhesive used to adhere polyester or nylon fibers (flock) to a variety of elastomers including EPDM, NR, CR, and SBR. Flocked substrates provi..
Density 0.977 g/cc
0.0353 lb/in³
Mixed
ITW Plexus Plexusâ„¢ MA420FS Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, very fast curing.Information provided by Illinois Tool Works.
Density 0.976 g/cc
0.0353 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON FX98500 PE
LNP* STAT-KON* FX98500 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Density 0.976 g/cc
0.0353 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific)
LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Density 0.976 g/cc
0.0353 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific)
LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Density 0.976 g/cc
0.0353 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON FX98500C PE
LNP* STAT-KON* FX98500C is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Density 0.978 g/cc

@Temperature 15.6 °C
0.0353 lb/in³

@Temperature 60.1 °F
ASTM D4052
ExxonMobil Exterex™ TM111 Synthetic Fluid
Product Description: Esterex™ Tirmellitate Esters are API category Group V fluids. These esters have excellent low-temperature properties, good lubricating properties and low volatilities. Esterex™..
Density 0.976 - 0.982 g/cc
0.0353 - 0.0355 lb/in³
BRCP 4843
ExxonMobil Jayflex™ TINTM Plasticizer
Appearance: Clear and FreeAvailability: North AmericaCAS Number: 53894-23-8Information provided by ExxonMobil
Density 0.976 g/cc
0.0353 lb/in³
BASF 1-Ethynyl-1-cyclohexanol
Formula: C8H12OCAS: 78-27-3Description: Ethynylcyclohexanol is a colorless solidified mass, with a faint specific odor.Synonyms: 1-EthynylcyclohexanolApplications: Intermediate used in the productio..
Density 0.977 g/cc
0.0353 lb/in³
BNZ Materials 2861LI Insulating Aggregate
BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i..
Density 0.977 g/cc
0.0353 lb/in³
Fired at 5 hrs at 816°C
BNZ Materials Bazelite 2300 LI Insulating Castable
Blaz 2300 L is similar to Blaz 2300 but suitable for those applications where reducing conditions might be encountered. These high purity, low iron products are specifically designed for both back-u..
Density 0.978 - 1.11 g/cc
0.0353 - 0.0401 lb/in³
Average value: 1.05 g/cc Grade Count:9
Overview of materials for Silicone Polyurethane, Ether Based
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value..