Physical Properties Metric English Comments
Density 0.950 - 1.00 g/cc

@Temperature 20.0 °C
0.0343 - 0.0361 lb/in³

@Temperature 68.0 °F
Hong Kun Group AO 1135 Antioxidant
This product is phenols antioxidant, applicable to the occasion that there are liquor, latex, soliquoid and mixture,especially applicable to polyols and polyurethane.it has excellent effect in anti-..
Density 0.900 - 1.00 g/cc

@Temperature 20.0 °C
0.0325 - 0.0361 lb/in³

@Temperature 68.0 °F
Grade A
Kazanorgsintez Polyalkylbenzene Resin
Production Method: Polyalkylbenzene resin is the by-product of isopropyl benzene production. Application: Intended for national economic needs and Grade A is exportedInformation Provided by Kazanorg..
Density 0.850 - 1.00 g/cc

@Temperature 20.0 °C
0.0307 - 0.0361 lb/in³

@Temperature 68.0 °F
Kazanorgsintez Pyrolysis Heavy Resin
Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis. Application: Used in the production of technical carbon, coak, and dark polymeric petroleum resin.Informa..
Density 0.250 - 1.00 g/cc
0.00903 - 0.0361 lb/in³
available range
MarkeTech Carbon Nanofoam
Electrically conductive carbon nanofoams possess many of the properties of traditional aerogel material. These materials are available in the form of monoliths, granules, powders and papers. They ar..
Density 0.980 - 1.00 g/cc
0.0354 - 0.0361 lb/in³
Wacker Silicones Geniomer® 140 Silicone TPE
SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas..
Density 0.980 - 1.00 g/cc
0.0354 - 0.0361 lb/in³
Wacker Silicones Geniomer® 200 Silicone TPE Elastomer
SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas..
Density 0.922 - 1.00 g/cc
0.0333 - 0.0361 lb/in³
Spec; ISO 1183-1
Axion Polymers Axpoly® PP06 5001 Enhanced Black General Purpose Polypropylene
PP06 Series polypropylene offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PP06 range of resin co..
Density 0.900 - 1.00 g/cc
0.0325 - 0.0361 lb/in³
Free Density
C.O.I.M. UREXTER® T 404 Polyurethane Two-Component Compound
Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc.
Density 0.980 - 1.00 g/cc
0.0354 - 0.0361 lb/in³
Wacker Silicones Geniomer® 80 Silicone TPE
SLM TPSE 80 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase..
Density 0.917 - 1.00 g/cc
0.0331 - 0.0361 lb/in³
Average value: 0.923 g/cc Grade Count:324
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi..
Density 0.980 - 1.00 g/cc
0.0354 - 0.0361 lb/in³
Wacker Silicones Geniomer® 60 Silicone TPE
SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase..
Copyright © lookpolymers.com All Rights Reserved