Physical Properties Metric English Comments
Density 0.935 - 1.02 g/cc

@Temperature 240 - 260 °C
0.0338 - 0.0368 lb/in³

@Temperature 464 - 500 °F
Average value: 0.981 g/cc Grade Count:16
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Density 1.02 - 1.02 g/cc

@Temperature 290 - 310 °C
0.0368 - 0.0368 lb/in³

@Temperature 554 - 590 °F
Average value: 1.02 g/cc Grade Count:10
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Density 1.02 - 1.02 g/cc

@Temperature 280 - 300 °C
0.0368 - 0.0368 lb/in³

@Temperature 536 - 572 °F
Average value: 1.02 g/cc Grade Count:6
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Density 1.01 - 1.02 g/cc
0.0364 - 0.0368 lb/in³
Mallard Creek Polymers TYLAC® 814 SBR Emulsion
Tylac® 814 is a surfactant stabilized styrene-butadiene copolymer latex. Features: when used in properly designed hydraulic cement mixtures, the addition of Tylac® 814 produces grouts, mortar..
Density 1.01 - 1.02 g/cc
0.0364 - 0.0368 lb/in³
Mallard Creek Polymers TYLAC® 873 Nitrile Emulsion
Tylac® 873 is a carboxylated acrylonitrile-butadiene copolymer latex. Features: good resistance to oil, grease and solvent, compatible with anionic asphalt emulsions, broadens the temperature ran..
Density 0.899 - 1.02 g/cc
0.0325 - 0.0368 lb/in³
Lord Adhesives 26 No-Mix Accelerator for 200/500 Series
Lord Adhesives 26 No-Mix Accelerator for 200/500 Series
Density 0.995 - 1.02 g/cc
0.0359 - 0.0368 lb/in³
Lord Adhesives 513 Fast Cure, Non-Sagging Acrylic Adhesive
Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi..
Density 0.971 - 1.02 g/cc
0.0351 - 0.0368 lb/in³
Lord Adhesives 660 White, Non Sag, Fast Set for FRP Acrylic Adhesive
Lord Adhesives 660 White, Non Sag, Fast Set for FRP Acrylic AdhesiveLord 660 Acrylic Adhesive bonds FRP (fiber-reinforced plastics) with minimal surface preparation. Lord 660 can cross-bond FRP to m..
Density 0.980 - 1.02 g/cc
0.0354 - 0.0368 lb/in³
ISO 1183
Austin Novel Materials Texalan® 765A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Density 0.960 - 1.02 g/cc

@Temperature 280 - 330 °C
0.0347 - 0.0368 lb/in³

@Temperature 536 - 626 °F
Average value: 1.01 g/cc Grade Count:43
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..
Density 1.01 - 1.02 g/cc
0.0365 - 0.0368 lb/in³