Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.00 - 1.04 g/cc | 0.0361 - 0.0376 lb/in³ | Average value: 1.02 g/cc Grade Count:26 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Density | 0.989 - 1.04 g/cc | 0.0357 - 0.0376 lb/in³ | 309-2D Hardener |
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh.. |
|||
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0376 lb/in³ | |
Silikony Polskie Silpasta A Silicone Paste Vaseline consistency, slightly thixotropicAntiadhesive agent used in thermoplastic and thermosetting processing to paste ground joints, rubber gaskets, etc. |
|||
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0376 lb/in³ | |
Silikony Polskie Silpasta E Silicone Paste Vaseline consistency, thixotropicElectric insulation to paste insulators, conductor connection, cable boxes in environment of high humidity or dustiness. |
|||
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0376 lb/in³ | |
Silikony Polskie Silpasta EM Silicone Paste Vaseline consistency, thixotropicElectric insulation for mechanical application of protective layers on electric devices and connections. |
|||
Density | 1.00 - 1.04 g/cc | 0.0361 - 0.0376 lb/in³ | RP-0549 |
Solvay AG-RHOâ„¢ FM 3896 Surfactant Description: Agricultural Foam Marker Concentrate. Very low alcohol content. Performs well in hard water up to 1000 ppmChemical Name: FOAM MARKER CONCENTRATE CAS: 111-76-2, 64-17-5 Solubility in Wat.. |
|||
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0376 lb/in³ | approximation |
Struktol STRUKSILON 8101 Silicone Stabilizer for PU-Rigid Foam STRUKSILON 8101 is used as a silicone stabilizer for production of polyurethane rigid foam. It is especially recommended for the use in PU-1- or PU-2-component spray foam applications.Applications: .. |
|||
Density | 0.960 - 1.04 g/cc | 0.0347 - 0.0376 lb/in³ | RP-0549 |
Solvay RHODATERGE® MULTIGREEN II Surfactant Description: Rhodaterge® Rhodaterge® Multigreen II is a general purpose Green Concentrate. It provides excellent oily soil removal for household, industrial and institutional products. It sis .. |
|||
Density | 0.900 - 1.04 g/cc | 0.0325 - 0.0376 lb/in³ | Average value: 0.920 g/cc Grade Count:278 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |
|||
Density | 0.930 - 1.04 g/cc | 0.0336 - 0.0376 lb/in³ | Average value: 0.957 g/cc Grade Count:16 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Compounding Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Compounding Grade". Each property range of values reported is minimu.. |
|||
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0376 lb/in³ | |
Silikony Polskie Silpasta Z Silicone Paste A consistency of hard VaselineLubricating agent to dampen vibrations in transmission gears and other mobile element made of plastic. |
|||
Density | 1.01 - 1.04 g/cc | 0.0365 - 0.0376 lb/in³ | |
Solvay RHODASURF® BC-840 Surfactant Chemical Name: TRIDECYL ALCOHOL ETHOXYLATEDCAS: 78330-21-9Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODASURF BC-840 is used for the following applications: f.. |
|||
Density | 1.03 - 1.04 g/cc | 0.0372 - 0.0376 lb/in³ | |
Solvay RHODASURF® ON-870 Surfactant Description: Rhodasurf® ON 870 is Ethoxylated Oleyl Alcohol. It is low foaming emulsifier. It is good wetting agent, dispersant, and detergent.Chemical Name: ETHOXYLATED OLEYL ALCOHOLCAS: 9004-98-2.. |
|||
Density | 0.886 - 1.04 g/cc | 0.0320 - 0.0376 lb/in³ | Average value: 0.905 g/cc Grade Count:61 |
Overview of materials for Polypropylene, Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values.. |