Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D-792 |
Plaskolite West Optix® CP - 80 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Asia Pacific) Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DI001L PC LNP* LUBRICOMP* DI001L is a compound based on Polycarbonate resin containing 2% Silicone. Added characteristics of this grade are: Low Extractable. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D-792 |
Plaskolite West Optix® CA - 51 KC General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
Plaskolite West Optix® CA-82 UVA UV-Absorbing Acrylic Resin Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for injection molding and contains a mold release agent. This resin offers high heat .. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics Lexan® 151 PC Nonhalogenated. 2.5 MFR. Blowmolding/extrusion.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 243 PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
Nilit FRIANYL B63 W-KV10 Nylon 6 for injection molding, 10% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP BG004 SAN (Europe-Africa-Middle East) LNP* LUBRICOMP* BG004 is a compound based on Styrene Acrylonitril resin containing Graphite. Added features include: Internally Lubricated. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 17% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | Injection molded parts; ASTM D792 |
Huntsman IROGRAN® PS455-200 TPU-Polyester Introduction: IROGRAN PS455-200 is a polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN PS455-200 is part of the HUNTSMAN film and sheet product range and offers.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP AF004AH ABS LNP THERMOCOMP* AF004AH is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Healthcare. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP PF002 PA 6 LNP THERMOCOMP* PF002 is a compound based on Nylon 6 resin containing 10% Glass Fiber. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF002XXH PA 66 LNP THERMOCOMP* RF002XXH is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added feature of this material includes: Healthcare. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Xenoy® XLG2400 PC+PET Low Gloss Xenoy, providing inherent low gloss on almLow Gloss Xenoy, providing inherent low gloss on almost every type of tool surfaces. This grade has excellent low temperature impact, high heat re.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183B |
Styron EMERGEâ„¢ 5302 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5302 is a black, 20% glass-filled ABS which is suitable for use in a wide variety of internal structural component applications in the information technology market. Applications: .. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
Eastman DuraStar MN620 Polymer, Natural Applications:Blood therapyDrug deliveryIV componentsMedicalSurgical instrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAProduct Description: DuraStar Poly.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
Covestro Desmopan® DP 2586A Polyurethane Extrusion- and injection molding gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentBeadsApplicationBlown filmsPreprocessingMax. Water co.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183-1 |
Covestro Makrolon® ET UV110 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• PC/UV absorber concent.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | |
DuPont Performance Polymers Delrin® 100PE BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE BK602 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
Covestro Makrolon® DP1-1825* Polycarbonate, Impact Grade Developmental productISO 7391-PC,MP,(,,)-09-9MVR (300 °C/1.2 kg) 6.0 cm3/10 minImpact modifiedHigh viscosityInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPreproce.. |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1183 |
Fainplast Compounds PG 7030 Flexible PVC, Extrusion Modified with Rubber Diesel Oil resistent profiles |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 490A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
Plaskolite West Optix® CA-68 General Purpose Acrylic Resin Injection Molding and Extrusion Grade. Good heat resistance, medium flow. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
PolyOne Elastamax XL 0254-15 TPU-Based Thermoplastic Elastomer
(discontinued **) This is a urethane based thermoplastic elastomer specially lubricated for auto suspension bushings. Physical Form: Pellets. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hann.. |