Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.20 g/cc | 0.0433 lb/in³ | |
Unifrax Fiberfrax® Rigidizer™ Inorganic Liquid Hardener Rigidizer™ and Rigidizer™ W, inorganic liquid hardeners, have a temperature grade rating of 1260°C (2300°F). They are generally used to increase the durability and surface erosion resistance of.. |
|||
Density | 1.20 g/cc | 0.0433 lb/in³ | |
Unifrax Fiberfrax® Rigidizer™ W Inorganic Liquid Hardener Rigidizer™ and Rigidizer™ W, inorganic liquid hardeners, have a temperature grade rating of 1260°C (2300°F). They are generally used to increase the durability and surface erosion resistance of.. |