Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
Nilit FRIANYL A63 HH-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® 104 PC (Europe-Africa-Middle East) LEXAN 104 is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatibility informati.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® EX1332T PC (Europe-Africa-Middle East) LEXAN* EX1332T polycarbonate resin, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, extrusion, mold release, UV stabilized, transparent, translucent and opaque colors. Multiwall sheet, Profi.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Europe-Africa-Middle East) 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer (Europe-Africa-Middle East) 19 MFR LEXAN High Flow Ductile Copolymer with 400 nm cut off, available in transparent colors only |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® HPS1S PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics Lexan® IFX2420Z PC (Asia Pacific) Lexan* IFX2420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware applications specifically for welding. This grades .. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® 925U PC (Europe-Africa-Middle East) Lexan* 925U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® HP6 PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mo.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon A4020-C004FR 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 15% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film FAR 25.853 Recognition: Product is des.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ASTM D792 |
Global PC-FR2 UL Recognized 94V-2 Polycarbonate Information provided by Global Polymers Corporation. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics PC0700 PC (Asia Pacific) PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A9600R Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON DD200C PC (Asia Pacific) PTFE free polycarbonate compounds with ESD safety and good lubricating perfomrance , suitable for Semiconductor and Hard Disk Drive (HDD) and semicon industry. Added features of this material includ.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ASTM D792 |
Lubrizol Isoplast® 2531 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | DIN 53479 |
Polyram RamTough RZ225 Polycarbonate, Injection Molding Polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | DIN 53479 |
Polyram RamTough RZ720 Polycarbonate, UV Stabilized UV stabilized and impact modified polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
Chengdu Polyster H6555 Thermoplastic Polyether-ester Elastomer (TPEE) Medium modulus molding and extrusion grade. Contains improved color- stable antioxidants. Good balance of modulus and toughness. Parts and components of automobile, hydraulic hose and slide of eleva.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
Chengdu Polyster KLX-G11 PC Film & Sheet PC film and sheet, high transparency, both sides are polished, both sides with transparent protective films. Is printable, flame-retardant, anti-static, resists ultraviolet decay, scratch resistant,.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
Covestro Makroblend® KU 2-7912 MBS151 Polycarbonate + PBT, Impact Grade (PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedAs of 1 September 2015, Bayer MaterialScience was separated.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183-1 |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
Covestro Makrolon® 6455 Polycarbonate, Flame Retardant Grade MVR (300 °C/1.2 kg) 12.5 cm3/10 minUL 94V-0/3.0 mmeasy releaseinjection moldingavailable in transparenttranslucent and opaque colorsPreprocessingMax. Water content |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | |
Covestro Makrolon® 6555 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding with easy mold release, burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG a.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
CP-Polymer-Technik Wellamid® 6000/42 GV 15 HWCP 15% Glass Fiber Nylon 6, Polymer Modified, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ASTM D792 |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
CENTROPLAST CENTROCARB Polycarbonate CENTROCARB is a transparent or semi-transparent plastic with high strength and impact resistance. It is dimensionally rigid and has very good electrical insulating properties. It is used in contain.. |