Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.26 g/cc | 0.0456 lb/in³ | Resin |
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures .. |
|||
Density | 1.26 g/cc | 0.0456 lb/in³ | Resin |
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin 4581 Astroquartz III Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures .. |
|||
Density | 1.26 g/cc | 0.0456 lb/in³ | Resin |
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin IM7 12K Carbon Uni-tape Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures .. |
|||
Density | 1.26 g/cc | 0.0456 lb/in³ | Resin |
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin T650-35-6K-UC309-5HS Carbon Fabric Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures .. |