Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.30 g/cc | 0.0470 lb/in³ | |
Plastcom SLOVAMID 6 GF 35 FRC 5 PA6 reinforced with 35% glass fibre, with flame retardant PA 6 for injection moulding, chemically reinforced with 35 % glass fibre, with halogen free flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 750°C, C.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | Crystalline; ISO 1183 |
Victrex® HT™ P45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion
compounding, low flow, FDA food contact compliant, co.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica.. |
|||
Density | 1.30 - 1.58 g/cc | 0.0470 - 0.0571 lb/in³ | Average value: 1.46 g/cc Grade Count:17 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | |
Haveg Havaflex T.A.-118 Phenolic, Trowelable Ablative Coating A two-component modified phenolic ablative coating and adhesive. This material was developed for the U.S. Army to protect the areas around missile launching systems from the extremely high heats (u.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
Lavergne VYPET PBT 6300 BK PBT Unreinforced, Impact Modified Vypet PBT 6300 BK is an unreinforced PBT injection molding compound offering excellent dimensional stability, chemical resistance, low moisture absorption and good electrical properties.Features: Hi.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific) LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ajedium™ Films -- Radel® R-5100 NT15 Polyphenylsulfone (PPSU) Radel® polyphenylsulfone is an amorphous thermoplastic material that offers exceptional hydrolytic stability, and toughness superior to other commercially available, high-temperature films. PPSU .. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK) AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK) KetaSpire® KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire® PEEK is produced to the highest industry standa.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC (Asia Pacific) LNP* STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing PTFE, Silicone, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied b.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF25 HS L BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF25 L BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
Shuman 930-05V0 White Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA6.10 LNP THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON DE006ER PC (Asia Pacific) LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL GFN3V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN3V is a 30 % glass fibre reinforced material with a HDT/A of 145C according ISO 75. NORYL GFN3V has been approved for potable water applications up to 85C by the UK WFBS according BS 6920 i.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
DSM Arnite® T08 200 (extrusion) PBT (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® 6134 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin 6134 NC010 is an unreinforced medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont .. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | Calculated from nominal thickness and yield |
DuPont Teijin Films Mylar® RL32 Polyester Packaging Film, 100 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL32 (formerly known as XM999) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | Calculated from nominal thickness and yield |
DuPont Teijin Films Mylar® RL32 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL32 (formerly known as XM999) is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a .. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183-1 |
Covestro Bayblend® FR410 MT Rubber Modified PC Blend, 10% Mineral Filled Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
Chem Polymer Chemlon 215 GVH Nylon 6, 15% Glass Fiber Reinforced A glass fiber reinforced, flame retardant nylon 6. The material has a V0 flammability rating according to UL 94 testing procedure at thicknesses down to 1/16" (1.57mm).Data provided by the manufact.. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
BASF Ultradur B 6550 PBT Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON RCL42 PA 66 (Europe-Africa-Middle East) LNP* Stat-kon* REL42 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
DSM Arnite® T06 202 PBT (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |