Physical Properties Metric English Comments
Density 1.15 - 1.35 g/cc
0.0415 - 0.0488 lb/in³
Average value: 1.21 g/cc Grade Count:8
Overview of materials for Glass Reinforced, Modified SMA
This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of..
Density 1.01 - 1.35 g/cc
0.0365 - 0.0488 lb/in³
Average value: 1.09 g/cc Grade Count:33
Overview of materials for Nylon 612, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp..
Density 1.04 - 1.35 g/cc
0.0376 - 0.0488 lb/in³
Average value: 1.11 g/cc Grade Count:8
Overview of materials for Nylon 11, Powder
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Powder". Each property range of values reported is minimum and maximum values of appropriate M..
Density 1.15 - 1.35 g/cc
0.0415 - 0.0488 lb/in³
Compounded
Butyl Rubber (IIR, CIIR, BIIR)
Butyl rubber is a copolymer of isoprene (minor) and isobutylene. Chlorobutyl (CIIR) and Bromobutyl (BIIR) contains 1.2% of the halogen. The halogen addition changes the cure characteristics and ca..
Density 1.31 - 1.35 g/cc
0.0473 - 0.0488 lb/in³
ISO R 1184
Fainplast Compounds RST 0413 Rigid PVC, Extrusion Lead Free
Transparent antishock profiles
Density 1.27 - 1.35 g/cc
0.0459 - 0.0488 lb/in³
Sibur 140-13 Compound 230/1 Polyvinyl Chloride (PVC)
Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p..
Density 1.29 - 1.35 g/cc
0.0466 - 0.0488 lb/in³
Dow BETAMATE™ 1045 Epoxy
BETAMATE™ 1045 is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excellent..
Density 1.31 - 1.35 g/cc
0.0473 - 0.0488 lb/in³
ISO R 1183
Fainplast Compounds CKL 90/40 Flexible PVC, Sheathing Lead Free
General purposes (75°C)
Density 1.31 - 1.35 g/cc
0.0473 - 0.0488 lb/in³
ISO R 1183
Fainplast Compounds GK 77/R Flexible PVC, Flame Retardant Sheathing Lead Free
Mineral oil resistant (90°)
Density 1.31 - 1.35 g/cc
0.0473 - 0.0488 lb/in³
ISO R 1184
Fainplast Compounds GS 7325 Flexible PVC, Electrical Plugs
Plugs
Density 1.31 - 1.35 g/cc
0.0473 - 0.0488 lb/in³
ISO R 1183
Fainplast Compounds GS 7325 Flexible PVC, Injection Molding for Technical Items
Plugs
Density 1.31 - 1.35 g/cc
0.0473 - 0.0488 lb/in³
ISO R 1184
Fainplast Compounds HL 96/1 Flexible PVC, Insulation for High Temperatures
Operating temperature 105°C
Density 1.31 - 1.35 g/cc
0.0473 - 0.0488 lb/in³
ISO R 1184
Fainplast Compounds KL 50 Flexible PVC, Insulation for High Temperatures Lead Free
Insulation for low thickness
Density 1.31 - 1.35 g/cc
0.0473 - 0.0488 lb/in³
ISO R 1184
Fainplast Compounds KL 93/1 Flexible PVC, Insulation for High Temperatures Lead Free
Operatine temperature 105°C
Density 1.31 - 1.35 g/cc
0.0473 - 0.0488 lb/in³
ISO R 1183
Fainplast Compounds PM 6640 Flexible PVC, Extrusion
Window gaskets
Density 1.20 - 1.35 g/cc
0.0434 - 0.0488 lb/in³
ISO 1183
BASF Ultradur® B 4500 BK 00110 PBT
Information provided by BASF
Density 1.15 - 1.35 g/cc
0.0415 - 0.0488 lb/in³
Compounded
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Nitrile Rubbers are copolymers of butadiene and acrylonitrile. The term has also been applied to copolymers of other dienes and/or nitriles. Acrylonitrile content may range from 18-50%. Increasin..
Density 1.31 - 1.35 g/cc
0.0473 - 0.0488 lb/in³
ISO R 1183
Fainplast Compounds PK 77/K-FR Flexible PVC, Lead Free
Flame retardant profiles exercise temp. 105°C