Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.37 g/cc | 0.0495 lb/in³ | STN 64 0111 |
Plastcom SLOVAMID 66 GF 35 FRG 5 Polyamide 66, 35% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 66 for injection moulding, chemical reinforced with 35% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
PTS Trimid® N66-G33HL 33% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
DSM Akulon® Ultraflow™ K-FHGM24 Nylon 6-30% Glass and Mineral Reinforced (European Grade) (Dry)
(discontinued The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG-K is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: Thi.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 718 V30 PA66, 30% glass fiber, DRY Description: TECHNYL A 718 V30 is a polyamide 66 reinforced with glass fiber and thermal stabilized for injection moldingColors: it is sailed on natural and black colorAvailable in: Latin AmericaMai.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP LL004E PEEK LNP* LUBRICOMP* LL004E is a compound based on Polyetheretherketone resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP LL004E PEEK (Asia Pacific) LNP* Lubricomp* LL004E is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Veradel® 3100P Polyethersulfone (PESU) Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Veradel® 3300 ULT Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability as well as resistance to steam, hot water and mineral a.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF30 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation p.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF30 L UV BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA 11 (Asia Pacific) LNP* THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing Glass Fiber. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP LF002 PEEK LNP* THERMOCOMP* LF002 is a compound based on Polyetheretherketone resin containing 10% Glass Fiber. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA11 LNP THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing 40% Glass Fiber. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | DIN 53479 |
Polyram PlusTek PA309G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, UV stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | |
Zoltek Pyron® Continuous Tow Oxidized Pan Fiber Oxidized Pan FiberApplications include: Yarn Stretch Breaking, Pulp Milling, Staple Fiber Chop for Nonwovens or Yarn Spinning |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | |
Zoltek Pyron® Satin Weave & Knit Fabric Oxidized Pan Fiber Oxidized Pan Fiber |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
Eurostar Staramide AG6H PA66, 30% Glass Filled, Injection Molded AG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
Eurostar Staramide RF006K PA66, Glass Fiber Filled, Injection Molded Staramide RF006K is a Radiation Crosslinkable, Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
Eurostar Starflam BFR330A PA6, Glass Bead Reinforced, Flame Retardant, Injection Molded Starflam BFR330A is a Flame Retardant, Glass Bead Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR10 NL PBT 10% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
BASF Ultraform® N2640 Z2 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Dry) Description: 20% mineral-filled and 10% glass-fiber reinforced injection-molding grade with outstanding flowability for technical parts with medium rigidity and high dimensional stability, e.g. for.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Conditioned) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
Chang Chun Plastic Longlite PM T33J General Purpose Phenolic Molding Compound ASTM Grades per ASTM D700 are 2,3.Information provided by Dowell Trading Company Ltd. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:.. |
|||
Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D-792 |
Sumitomo Bakelite North America FM 1132P Cellulose Reinforced Phenolic Novolac FM 1132P is a two-stage phenolic molding compound reinforced with cellulose in pellet form. FM-1132P is recommended to customers desiring approval under ASTM D-5948-96,Type CFI-10. (Replaces Militar.. |