Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.46 g/cc | 0.0527 lb/in³ | |
Plastcom SLOVAMID 66 CF 40 PA66, 40% carbon fibre FeaturesChemically reinforced with 40% carbon fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. .. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183-1 |
Quadrant EPP Acetron® MD POM-C + metal detectable additive, extruded (ISO Data) Metal detectable POM-C grade High mechanical strength, stiffness and hardness Excellent resilience Good creep resistance High impact strength, even at low temperatures Very good dimensional stabilit.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Shell Carilon® DB6G6A10 Polyketone, 30% Glass-Reinforced General-Purpose Injection Molding Grade
(discontinue Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6G6A10 is a 30 percent short glass-fiber-reinforced, general purpose injection molding grade, wit.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
DSM Akulon® K224-G8U (Dry) 43% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Density | 1.46 - 1.99 g/cc | 0.0527 - 0.0719 lb/in³ | Average value: 1.58 g/cc Grade Count:32 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1184 |
Fainplast Compounds RKS 325 Rigid PVC, Antishock Extrusion Lead Free Various profiles, antishock |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Lanxess Durethan® BM 240 H2.0 901510 Nylon 6, 40% Mineral PA 6, injection molding grade, 40% mineral, isotopic properties, good heat-ageing resistance |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Techmer ES Elastoblend® PA6 GF40 IM2 NAT 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP UX95672 PPA LNP LUBRICOMP* UX95672 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PA6 GF40 ML5 HS 12 mm 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilized and Molybdenum Disulfide LubricantFeatures: Lubricated and Heat StabilizerAp.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PA6/6 GF30 IM TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resi.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PA6/6 GF33 TL10 HS 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance, Heat Stab.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RF008XXZ PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF008XXZ is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOTUF RF008IS PA 66 LNP* Thermotuf* RF008IS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Vyncolit Vyntec® CF8131 Carbon Fiber Reinforced Phenolic VYNTEC CF8050 is a carbon fiber reinforced phenolic moldable composite with good tribological and superior mechanical properties combined with low density. Very good chemical resistance in several o.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Tisan TISESTER® 30% Glass Fiber Reinforced, Impact Resistance and Heat Stabilized ISI Stab. Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Wellman Wellamid® MRGF30/10 42H-N 30% Mineral/10% Glass Fiber Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183-87 |
Wellman Wellamid® MRGFX1716-BK1 40% Mineral/Glass Reinforced, Silicone Lubricated Nylon 6 Description: Mineral/Glass Reinforced, Silicone Lubricated Nylon 6Information provided by Wellman. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Polyram RamTal PM3007G2 Polyacetal for Injection Molding, 10% Glass Fiber Reinforced 10% Glass fiber reinforced polyacetal for injection molding applications.Information provided by Polyram. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | DIN 53479 |
Polyram RamTal PM7013G2 Acetal, 10% Glass Fiber 10% Glass fiber reinforced and UV stabilized polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | |
DuPont™ Kapton® 100EN Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)Kapton® Type E and EN films have superior dimensional stability, low CHE, a CTE close to copper, and a high modulus. This type is exceptional for applications req.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® S650FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Flame Retardant Polybutylene Terephthalate Crastin S650FR is an unreinforced flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance .. |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 92 Flexible PVC, Insulation General purposes |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 039/31 Halogen Free PVC Sheathing, insulation; high flexibility |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 76/2 Flexible PVC, Sheathing General purposes |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183/A |
Addiplast Addinyl A2 ZV40 Nylon 66, 40% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Conditioned, 40% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Plenco 7591 Phenolic, Pellet, Transfer Molded PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |