Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
Lanxess Durethan® BKV 50 H2.0 EF 000000 Nylon 6, 50% Glass Fiber PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance, low viscosity (easy flow) |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF50 HS UV BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF50 IM 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingIn.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF50 IM L NAT001 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricated and Impact ModifiedProcessin.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF50 L BN047 LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedAppearance: BeigeInformation.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF50 HS L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformati.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF50 HS L BK 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF50 L UV 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformat.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
Stir SpA AF 90/1 (PVC) Application: Flame resistant sheath CEI 20-11 RZInformation provided by STIR SpA |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP KF004AL Acetal Homopolymer LNP* THERMOCOMP* KF004AL is a compound based on Acetal Homopolymer resin containing 20% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RF00ASXS PA6.6 (Europe-Africa-Middle East) LNP* Thermocomp* RF00ASXS is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | GB/T 1033.1-2008 |
Sichuan Deyang Haton® hXGR41 Polyphenylene Sulfide Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RZ0069 PA 66 LNP* THERMOCOMP* RZ0069 is a compound based on Nylon 66 resin containing 30% Milled Glass. Added features of this material include: Flame Retardant. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RV00AEXP PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AEXP is a compound based on PA 66 resin containing Long Glass Fiber. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183-87 |
Wellman Wellamid® GFX1743-BK1(PTFE) 45% Glass Fiber Reinforced, Enhanced Lubrication Nylon 66/6 Description: Glass Fiber Reinforced, Enhanced Lubrication Nylon 66/6Information provided by Wellman. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | |
Trelleborg Emerson & Cuming Eccobond® 91 Two-Component High Strength-Peel Epoxy Adhesive Emerson & Cuming 91 Eccobond® Two-Component High Strength-Peel Epoxy AdhesiveFiberglass filled, medium viscosity, epoxy adhesive with excellent thermal cycling properties. Used with a variety of ca.. |
|||
Density | 1.57 g/cc @Temperature 23.0 °C |
0.0567 lb/in³ @Temperature 73.4 °F |
DIN 53 479 |
Ensinger TECASINT 5051 Polyimide, 30% Glass Fiber Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Density | 1.57 g/cc @Temperature 23.0 °C |
0.0567 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon 44981R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene UL Recognition File: E54153.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36E PC LNP LUBRICOMP* DFL36E is a compound based on Polycarbonate resin containing 30% Glass Fiber, 155 PTFE. Added features of this material include: Easy Molding, Internally Lubricated. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Covestro Petlon® 3530 Semi-Crystalline PET, 30% Glass Fiber
(discontinued **) Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Underhood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperatu.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® FG530 NC011 PET
(Unverified Data**) Rynite® FG530 NC011is a 30% glass fiber reinforced modified polyethylene terephthalate resin. It has been developed for consideration into applications for the food industry.Information provided by.. |