Physical Properties Metric English Comments
Density 1.23 - 1.62 g/cc
0.0444 - 0.0585 lb/in³
Average value: 1.34 g/cc Grade Count:5
Overview of materials for Polyphenylene Ether, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Mineral Filled". Each property range of values reported is minimum and maximum valu..
Density 1.29 - 1.62 g/cc
0.0466 - 0.0585 lb/in³
Average value: 1.41 g/cc Grade Count:17
Overview of materials for Acetal Copolymer, Silicone Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values..
Density 0.880 - 1.62 g/cc
0.0318 - 0.0585 lb/in³
Average value: 1.34 g/cc Grade Count:85
Overview of materials for PVC, Uncompounded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate ..
Density 1.08 - 1.62 g/cc
0.0390 - 0.0585 lb/in³
Average value: 1.48 g/cc Grade Count:18
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is ..
Density 1.20 - 1.62 g/cc
0.0434 - 0.0585 lb/in³
Average value: 1.38 g/cc Grade Count:81
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
Density 1.39 - 1.62 g/cc
0.0502 - 0.0585 lb/in³
Average value: 1.51 g/cc Grade Count:45
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Density 1.23 - 1.62 g/cc
0.0444 - 0.0585 lb/in³
Average value: 1.39 g/cc Grade Count:45
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
Density 1.58 - 1.62 g/cc
0.0571 - 0.0585 lb/in³
ISO R 1184
Fainplast Compounds RE 240 Rigid PVC, Extrusion
Electric channels
Density 1.58 - 1.62 g/cc
0.0571 - 0.0585 lb/in³
IEC 60811
Fainplast Compounds HAX HF 019/HT6 Halogen Free PVC
High fire performances, good flexibility
Density 1.60 - 1.62 g/cc
0.0578 - 0.0585 lb/in³
Beijing Evergrow Resources CFC-DD-1000 Carbon Fiber Cloth
The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro..
Density 1.60 - 1.62 g/cc
0.0578 - 0.0585 lb/in³
Beijing Evergrow Resources CFC-DD-1000S Carbon Fiber Cloth
The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro..
Density 1.60 - 1.62 g/cc
0.0578 - 0.0585 lb/in³
Beijing Evergrow Resources CFC-DDX-1000S Carbon Fiber Cloth
The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro..
Density 1.55 - 1.62 g/cc
0.0560 - 0.0585 lb/in³
Molding; IS 867-1963
Amity Thermosets ATS 131 Phenolic Molding Organic and graphite Filler, Compression Molded
Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti..
Density 1.60 - 1.62 g/cc
0.0578 - 0.0585 lb/in³
Beijing Evergrow Resources CFC-DDX-1000 Carbon Fiber Cloth
The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro..
Density 1.58 - 1.62 g/cc
0.0571 - 0.0585 lb/in³
ISO R 1184
Fainplast Compounds RE 224 Rigid PVC, Extrusion
Various profiles
Density 1.58 - 1.62 g/cc
0.0571 - 0.0585 lb/in³
ISO R 1184
Fainplast Compounds RE 430 Rigid PVC, Extrusion
Electric channels
Density 1.47 - 1.62 g/cc
0.0531 - 0.0585 lb/in³
Average value: 1.51 g/cc Grade Count:27
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Density 1.58 - 1.62 g/cc
0.0571 - 0.0585 lb/in³
ISO R 1184
Fainplast Compounds RE 230/D Rigid PVC, Extrusion
Electric channels