Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0589 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.32 - 1.63 g/cc
0.0477 - 0.0589 lb/in³
Average value: 1.42 g/cc Grade Count:51
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Density 1.42 - 1.63 g/cc
0.0513 - 0.0589 lb/in³
Average value: 1.48 g/cc Grade Count:77
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Density 1.20 - 1.63 g/cc
0.0434 - 0.0589 lb/in³
Average value: 1.34 g/cc Grade Count:121
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Density 1.15 - 1.63 g/cc
0.0415 - 0.0589 lb/in³
Average value: 1.36 g/cc Grade Count:85
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Density 1.59 - 1.63 g/cc
0.0574 - 0.0589 lb/in³
ISO R 1184
Fainplast Compounds RE 241 Rigid PVC, Extrusion
Various profiles
Density 1.59 - 1.63 g/cc
0.0574 - 0.0589 lb/in³
ISO R 1184
Fainplast Compounds RK 435 Rigid PVC, Extrusion Lead Free
Electrical channels
Density 1.38 - 1.63 g/cc
0.0499 - 0.0589 lb/in³
Average value: 1.48 g/cc Grade Count:39
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..