Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
LNP Lubricomp® PDX-O-90351 Polyphenylene Sulfide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | DIN 53479; ASTM D792 |
Kolon KOPET® KP132G30VO FR-PET Resin KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
Lanxess Pocan® T 7391 000000 PBT + PET, 45% Glass Fiber PBT+PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP OX90351 PPS LNP LUBRICOMP* OX90351 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP RFN169 PA 66 LNP* LUBRICOMP* RFN169 is a compound based on Nylon 66 containing 30% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant, Flame Retardant. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® FC-1150 Polyphthalamide (PPA), 50% Glass Fiber Amodel® FC-1150 is an FDA-approved, 50% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
Techmer ES HiFill® ABS 1067 Availability: North AmericaFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityForms: PelletsProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF60 IM HS L 60% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
Techmer ES HiFill® POM HO 0167 S1 Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: HomopolymerInformation provided by TP Composites, Inc. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PET GF30 FR X 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PEI GF30 TL15 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | |
UCAR Carbon UCAR® CBY Extruded Graphite Grade CBY is a general purpose, cost effective extruded graphite with improved strength, structure and density characteristics. It is a low ash graphite for superior oxidation resistance.Typical App.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
DSM Arnite® AV2 370 XL-T PET-GF35 35% Glass Reinforced, Low Outgassing, Thermal conductive material |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK695FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
Barlog Plastics KEBAFLOW MX130 LCP, 30% glass fiber / mineral reinforced LCP-GF/MD 30Information provided by BARLOG plastics GmbH. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
BASF Petra® 330 FR BK-112 30% Glass Filled PET Petra 330 FR BK-112 is a 30% glass reinforced, flame retardant PET, pigmented black injection molding compound rated UL94 V-0 in a 1/64 inch thickness. The product is designed for injection molding.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | |
A. Schulman ComAlloy Comtuf® 464 Glass Reinforced, Impact Modified, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | |
A. Schulman ComAlloy Hiloy® 617 Nylon 6, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.55% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
Bulk Molding Compounds BMC 665 Mineral Filled, Glass Reinforced Polyester BMC 665 molding compound is a mineral filled, glass reinforced polyester molding compound suitable for compression, transfer or stuffer injection molding. It is characterized by good moldability, o.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | |
LATI Latilub 80-17ST G/30 PPS, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). Silicone / PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 31T1 MZ40 PA66, 40% mineral fiber, DRY Description: Flame retardant polyamide PA66, 40% mineral filled, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | |
Pyrotek Pyroboard™ S800 Roller Pyroboard™ S800 is used in cooling areas of the furnace. Economically priced, S800 wears well and is designed to be used in the water quench cooling sections.Information provided by Pyrotek. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Conditioned) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |