Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.69 g/cc | 0.0611 lb/in³ | ASTM D792 |
Owens Corning Glass Fiber Reinforced Polyester (Pultruded), 55 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Density | 1.69 - 1.88 g/cc | 0.0611 - 0.0679 lb/in³ | Average value: 1.78 g/cc Grade Count:105 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO R 1183 |
Multibase Multibatch® ME 50003 Anti-blocking Masterbatch LDPE. 70% CaCO3 Filled. Anti-slipInformation provided by Multibase |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched LNP* LUBRICOMP* OFL36A is a compound based on PPS - Branched resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched LNP* LUBRICOMP* OFL36A is a compound based on PPS - Branched resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched (Europe-Africa-Middle East) LNP LUBRICOMP* OFL36 is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched (Europe-Africa-Middle East) LNP LUBRICOMP* OFL36 is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS (Asia Pacific) LNP* Lubricomp* OFL36A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183/A |
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66 LNP* THERMOCOMP* RFB66 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 30% Glass Bead. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RV0079 PA 66 (Asia Pacific) LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing Flame Retardant, Long Glass Fiber, Long Glass. Added features of this material include: Easy Molding. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON RX04493D PA 66 LNP* VERTON* RX04493D is a compound based on Nylon 66 resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
Vyncolit TX10916/15 Graphite Filled Novolac Phenolic Novolac resin based, graphite filled compound used for low friction applications where dimensional stability is requiredInformation provided by Sumitomo Bak North America, Inc. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | |
Covestro Baygal® 90 IK 69 Polyurethane Uses: Suitable for impregnation and encapsulation of coils, especially when high heat deflection temperature, and eventually fire resistance is requested.Information provided by Bayer.As of 1 Septem.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GV-6 FWA nat PA*-GF60 Product description: Grivory GV-6 FWA natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | dry; ISO 1183 |
DSM Stanyl® TW278F10 (PA46+PTFE)-GF50 50% Glass Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | |
Dow Saran® 313 PVDC SARAN® 313 barrier polymer, a copolymer of vinylidene chloride and vinyl chloride, is designed for extrusion and coextrusion into barrier films used in flexible packaging applications for food. It .. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GV XE 16102 (GVL-6H HP) PA*-GF60 Product description: Grivory XE 16102 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long special glass fibers. Grivory.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GV-6H black PA*-GF60 Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GVL-6H black 9839 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GVX-6 H nat PA*-GF60 Product description: Grivory GVX-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
Eurotec® Tecopet® PT74 GR45 BK002 PR PET, 45% glass fiber reinforced, high heat stabilized, black Information provided by Eurotec® |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
DSM Arnite® TV4 260 S PBT-30% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GV-6H EF nat PA*-GF60 Product description: Grivory GV-6H EF black 9915 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GV-6H PA*-GF60 Product description: Grivory GV-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide... |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069XZ PA 66 LNP THERMOCOMP* RF0069XZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |