Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
Multibase Multi-Pro® 7518 C Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
Plenco 51045 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is It is UL listed and available in black only.Information supplied b.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
Plenco 51130 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51130 is an engineering grade UL flame rated glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in black only.Inform.. |
|||
Density | 1.72 - 1.82 g/cc | 0.0621 - 0.0658 lb/in³ | Average value: 1.79 g/cc Grade Count:10 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | DIN 53 47 |
Albis Plastics Tedur® L 9512 PPS, 45% Glass Fiber
(discontinued **) Good-flow Embedding Compound. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Embedding of Microchips and Electronic ComponentsProcessing: Injection Molding (Melt Temp.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO R 1183 |
Multibase Multibatch® MP 52206 Sheet Extrusion HPP. 70% CaCO3 FilledInformation provided by Multibase |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | |
LATI Latilub 80-10T G/40 PPS, 40% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Density | 1.72 g/cc @Temperature 25.0 °C |
0.0621 lb/in³ @Temperature 77.0 °F |
|
Solvay Specialty Polymers Galden® SV135 PFPE Solvent Galden® SV grades are specifically recommended for use as solvents.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP PF00C PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PF00C is a compound based on PA6 resin containing Glass Fiber. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF00BS PA 66 (Asia Pacific) LNP* Thermocomp* RF00BS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp RF00CS PA 66 LNP* Thermocomp* RF00CS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RX12402 PA 66 LNP* Thermocomp* RX12402 is a compound based on PA66 containing 60% Glass Fiber. Added feature is Superior Flow. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific) LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
Solvay TECHNYL® 2912GMH7-P PA66, 63% glass fiber, DRY Description: Polyamide 66, reinforced with 63% of glass fiber for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2912GMH7-P is used in all sectors of industry, offerin.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | |
Cosmic Plastics K61 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK609 NC010 PBT
(Unverified Data**) Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-61L Compression Molded PPS Compound, 25% Fiberglass and Mineral Filled Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-64B Compression Molded PPS Compound, 40% Fiberglass, Black Pigmented Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)
(Unverified Data**) 60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
Eurostar Starflam RF023P PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam RF0023P is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding (also known as Starflam PA66C U2 Z23)Information provided by Eurostar. |
|||
Density | 1.72 g/cc @Temperature 23.0 °C |
0.0621 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | |
BASF Paliotol™ Yellow L 2140 Color Additive Description: Isoindoline yellow with high opacity and reddish shade for OEM and industrial coatings.Suitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing system, A.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Conditioned, 60% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Density | 1.72 g/cc @Temperature 40.0 °C |
0.0621 lb/in³ @Temperature 104 °F |
Liquid |
3M Novec™ 774 Engineered Fluid 3M™ Novec™ 774 Engineered Fluid is a clear, colorless and low odor fluid, and is one in a line of 3M products designed as replacements for ozone depleting substances (ODSs) and compounds with high.. |
|||
Density | 1.72 - 1.92 g/cc | 0.0621 - 0.0694 lb/in³ | Molded |
Bulk Molding Compounds BMC T40(18)V0 Die Casting Replacement Grade Molding Compound BMC T40(18)V0 is a lower cost version of BMC T40(18) where a UL 5V rating is not necessary. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
Sumitomo Bakelite North America RX® 680 Fiberglass and Glass Reinforced Phenolic RX 680 is a fiberglass and glass bead filled phenolic molding compound, with good dimensional stability and good strength at elevated temperatures.Information provided by Sumitomo Bak North America,.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
Plenco 50045 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s.. |