Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.75 g/cc | 0.0632 lb/in³ | ISO 1183/A |
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional cree.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Solef® 32008 PVDF Copolymer
(Unverified Data**) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
Quantum Composites QC-8100 60% Glass Fiber Vinyl Ester SMC
(discontinued **) QC-8100 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength and corrosion resistance. Form and Colors = Rolled Shee.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
Chevron Phillips Ryton® BR42C Polyphenylene Sulfide Compound
(discontinued **) Black Polyphenylene Sulfide CompoundRyton® BR42C is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surface fric.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | |
IDI Composites E-205 Thermoset Polyester, Sheet ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D572 |
Haysite 42000 Polyester SMC, 22% Glass Reinforced The 42000 series sheet molding compound is an electrical grade designed for compression molded parts requiring high strength and good electrical properties. This material possesses excellent moldabi.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KFL36 Acetal Copolymer LNP* LUBRICOMP* KFL36 is a compound based on Acetal Copolymer resin containing 30% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP RFL449 PA 66 LNP* LUBRICOMP* RFL449 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Flame Retardant. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ajedium™ PVDF 9009 Polyvinylidene Fluoride (PVDF) Solef® 9009 PVDF homopolymer is a semi-crystalline fluoropolymer. Solef® film is chemically inert to most acids, aliphatic and aromatic organic compounds, chlorinated solvents and alcohols.Fea.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA), 60% Glass Fiber Amodel® A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional .. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 1006 Polyvinylidene Fluoride (PVDF) Solef® 1006 PVDF is a very low viscosity homopolymer resin mainly used in injection molding or in multifilament extrusion.Features: Homopolymer; Low ViscosityUses: General PurposeAdditional Prope.. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF) Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Density | 1.75 - 1.80 g/cc | 0.0632 - 0.0650 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PBT GF30 CF10 FR 30/10% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber, 30/10% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 5C004 PVDF (Asia Pacific) LNP* Thermocomp* 5C004 is a compound based on Polyvinylidene Fluoride resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America 51-01 CAFR-P Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 2C004 ETFE LNP* THERMOCOMP* 2C004 is a compound based on ETFE resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | |
Toho Tenax Besfight® G30-500 12K HTA-7C NS01 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | |
Toho Tenax Besfight® G30-500 6K HTA-7C EP03 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | |
Hexcel® IM4 Carbon Fiber (12,000 Filaments) Weight/length = 0.723 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
Unitika RUN35-TA Light resistant PA6, Conditioned Light resistant and internalInformation provided by Unitika Ltd. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | |
Brandenburger BL 20/1 GG EP Rotor Blade Material BL 20/1 GG EP is a composite bearing material that combines the crucial parameters for rotary blades. These include compressive stability at high temperatures, impact strength, low swelling and low.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 Method A |
Arlon 49N Multifunctional Epoxy Low-Flow Prepreg 49N is a low-flow epoxy prepreg engineered for bonding multilayer epoxy rigid-flex or attaching heat sinks to multilayer PCBs. With a high Tg, the prepreg can be used in high-performance or high-te.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ISO 1183 |
BASF Ultramid® HMG14 HS BK 102 60% Glass Filled PA66 (Conditioned) Description: Ultramid HMG14 HS BK-102 is a 60% glass reinforced, injection molding grade of PA66 offering high strength and stiffness. Due to inherently lower moisture absorption, Ultramid HMG14 HS .. |
|||
Density | 1.75 - 1.95 g/cc | 0.0632 - 0.0704 lb/in³ | Molded |
Bulk Molding Compounds BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound BMC HT12-1023L is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid cap.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 Method A |
Arlon 47N Quick Cure Epoxy Low-Flow Prepreg 47N is a low-flow epoxy prepreg engineered for binding multilayer epoxy rigid-flex or attaching heat sinks to multilayer PCBs. An optional low lamination temperature protects components already mou.. |
|||
Density | 1.75 g/cc | 0.0632 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s). |
|||
Density | 1.75 - 1.85 g/cc | 0.0632 - 0.0668 lb/in³ | ASTM D792 |
Premix Premi-Glas® 1200-28 Polyester SMC
(discontinued **) Premi-Glas® 1200-28 series is a low profile, 28 % glass reinforced polyester Sheet Molding Compound designed for recreational vehicle body panels applications that require excellent flexibility and.. |