Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0640 g/cc | 0.00231 lb/in³ | |
Pyrotek L4 Fiber Seal Pre-cut Gasket A lightweight needled blanket which is strong and durable.Information provided by Pyrotek. |
|||
Density | 0.0640 g/cc | 0.00231 lb/in³ | |
Pyrotek L-4 Fiberseal Blanket Lightweight, yet strong and durable needled blankets.Dimensions610 mm x 7.6 m1219 mm x 7.6 m6 - 51 mm thickApplicationsFurnace linings Gaskets Expansion joints Fire blanket Fire pillowsInformation p.. |
|||
Density | 0.0640 g/cc | 0.00231 lb/in³ | |
Pyrotek M-2 Fiber Seal Pre-cut Gasket A light-brown ceramic fiber material. Excellent trough gasket material.Information provided by Pyrotek. |
|||
Density | 0.0640 g/cc | 0.00231 lb/in³ | |
Pyrotek M-2 High-Temperature Felt A light-brown material.Dimensions457 mm x 7.6 m 25 mm thickApplicationsHigh-temperature gasketsInformation provided by Pyrotek. |
|||
Density | 0.0640 - 0.0860 g/cc | 0.00231 - 0.00311 lb/in³ | sheet density |
Zotefoams Plastazote® HL79 Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0640 g/cc | 0.00231 lb/in³ | Molded density, ASTM D1622 |
Covestro Bayfill® EA 2003 Polyurethane Energy-Absorbing Semi-Rigid Foam, Friable Grade, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Density | 0.0640 g/cc | 0.00231 lb/in³ | Molded density, ASTM D1622 |
Covestro Bayfill® EA 6004 Polyurethane Energy-Absorbing Semi-Rigid Foam, Recoverable Grade, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Density | 0.0640 g/cc | 0.00231 lb/in³ | ASTM D3574A |
Covestro Bayfit® SA Polyurethane Sound Absorbing Foam, High-Resilience, Higher density Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Density | 0.0640 g/cc | 0.00231 lb/in³ | DIN 53420 |
Dow STRANDFOAM™ EA 1600 Polypropylene Foam STRANDFOAM™ EA 1600 Energy Absorbing polypropylene foam is a strong, low-density, closed-cell foam. It is suited as a component material in products requiring a shock and energy absorbing or vibra.. |
|||
Density | 0.0640 g/cc | 0.00231 lb/in³ | |
3M 4466B Double Coated Polyethylene Foam Tape 3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces in.. |
|||
Density | 0.0640 g/cc | 0.00231 lb/in³ | |
3M 4466W Double Coated Polyethylene Foam Tape 3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces in.. |
|||
Density | 0.0640 g/cc | 0.00231 lb/in³ | |
3M 4496B Double Coated Polyethylene Foam Tape 3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces in.. |
|||
Density | 0.0640 g/cc | 0.00231 lb/in³ | |
3M 4496W Double Coated Polyethylene Foam Tape 3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces in.. |
|||
Density | 0.0640 - 0.0760 g/cc | 0.00231 - 0.00275 lb/in³ | |
Akzo Nobel Expancel® 461 DE 20 d70 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0640 g/cc | 0.00231 lb/in³ | |
Pyrotek M-4 Fiberseal Blanket A white high-temperature felt.Dimensions610 mm x 15.2 m25 mm thickApplicationsGaskets Trough covers Trough gaskets Information provided by Pyrotek. |