Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.02 g/cc | 0.0730 lb/in³ | |
Meilian Chemical PE12086 WHITE MASTERBATCH WHITE PE12086 is a white low density polyethylene based masterbatch highly-concentrated with TiO2 without any addition of filler and fluorescence whitener. This product is designed for general-purpo.. |
|||
Density | 2.02 g/cc | 0.0730 lb/in³ | ASTM D792 |
Techmer ES HiFill® PP 0202 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Density | 2.02 g/cc | 0.0730 lb/in³ | ASTM D792 |
Plenco 1510 Polyester, Pellet, Injection Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |
|||
Density | 2.02 g/cc | 0.0730 lb/in³ | ISO 1183 |
Polyplastics Freqtis® C0711A (PPS/LCP), Molding Compound Both base resins (PPS and LCP) exhibit excellent heat resistance, dimensional stability and molding processability. Therefore Freqtis® is widely used for surface mounted electronic components. In .. |
|||
Density | 2.02 - 2.06 g/cc | 0.0730 - 0.0744 lb/in³ | ISO R 1183 |
Fainplast Compounds CRKA 90 Flexible PVC, Flame Retardant Electrical Bedding Lead Free Bedding non contaminating on XLPE |
|||
Density | 2.02 g/cc | 0.0730 lb/in³ | ASTM D792 Method A |
Arlon CLTE-XT High Precision Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing .. |
|||
Density | 2.02 g/cc | 0.0730 lb/in³ | |
AMT AM-Lite® Die Casting Magnesium Alloy AM-lite is a high surface finish die casting alloy suitable for applications that currently utilize zinc, aluminum or magnesium (alloy AZ91D) die castings, or plastic injection moldings. AM-lite has.. |
|||
Density | 2.02 g/cc | 0.0730 lb/in³ | |
BASF Paliotol™ Yellow L 0962 Color Additive Description: Opaque quinophthalone yellow with excellent rheologySuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing system and Airdrying systemsInformation prov.. |