Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.128 g/cc | 0.00462 lb/in³ | |
Pyrotek M-8 Fiber Seal Pre-cut Gasket Contains no binders and is not changed by exposure to high temperatures.Information provided by Pyrotek. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ N231XS 100% Neoprene Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Folded |
Unifrax Anchor-Loc® 2200 Ceramic Fiber Modules The Anchor-Loc® module system is a family of ceramic fiber module products designed to meet a wide range of application requirements in a variety of heat processing vessels.Ceramic fiber modules us.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Edge Grain |
Unifrax Fibermass® 2200 Ceramic Fiber Blocks Fibermass® ceramic fiber blocks combine advancements in fiber chemistry and manufacturing technology to provide an economical lining material for a wide range of heat processing equipment. The Fib.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | |
Unifrax Fibermax® Needled Blanket Fibermax® Needled Blankets are high temperature, light weight and flexible products manufactured from polycrystalline mullite fiber that can be exposed to temperatures up to 1600°C (2912°F). Fib.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Installed Fired |
Unifrax Foamfrax® Grade I Fiber Insulation Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic b.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Installed Fired |
Unifrax Foamfrax® Grade III Fiber Insulation Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic b.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Installed Fired |
Unifrax Foamfrax® Isofoam Fiber Insulation Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic b.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | |
Unifrax FyreWrap® MAX 2.0 Duct Insulation Two-Layer ASTM E-2336 System Unifrax's FyreWrap® MAX 2.0 Duct Insulation is a high-temperature insulation blanket specifically designed to provide a flexible enclosure for one- and two-hour rated commercial kitchen grease duct.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | |
Hexcel® HexWeb® HRH-327 - 3/16 - 8.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | |
Hexcel® HexWeb® HRP - 3/16 - 8.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Density | 0.128 g/cc | 0.00463 lb/in³ | Available |
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator Fiberfrax Durablanket 2600 insulation extends the high-temperature performance of the Durablanket product line. The product is made from high-purity alumina, zirconia, and silica spun ceramic fiber.. |
|||
Density | 0.128 g/cc | 0.00462 lb/in³ | |
Zircar Refractory Composites ASPA-2 Alumina-Silica Fiber Paper ASPA-2 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c.. |
|||
Density | 0.128 - 0.208 g/cc | 0.00463 - 0.00752 lb/in³ | |
Monmouth Rubber & Plastics Durafoam™ DK4141 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |