Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.00 - 7.20 g/cc | 0.253 - 0.260 lb/in³ | |
Pacific Sintered Materials F-241-S2 Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores.Equivalent ASTM Specification: B310-70, TYPE IV, CLASS AAll information provided by Pa.. |
|||
Density | 7.00 - 7.20 g/cc | 0.253 - 0.260 lb/in³ | |
Pacific Sintered Materials FN-251-S Invar Powdered Metal Coefficient of thermal expansion equal to glass.All information provided by Pacific Sintered Metals. |
|||
Density | 7.00 - 7.20 g/cc | 0.253 - 0.260 lb/in³ | |
Pacific Sintered Materials FN-252-S Iron Nickel Soft Magnetic Powdered Metal Very low coercive force and high permeability. Excellent for shielding and switching applications.All information provided by Pacific Sintered Metals. |
|||
Density | 7.00 - 7.20 g/cc | 0.253 - 0.260 lb/in³ | |
Pacific Sintered Materials FP-1650-S Phosphorous Iron Soft Magnetic Powdered Metal For applications requiring high yield strength and toughness. Magnetic properties superior to iron, but slightly inferior to silicon iron.All information provided by Pacific Sintered Metals. |
|||
Density | 7.00 - 7.30 g/cc | 0.253 - 0.264 lb/in³ | |
Pacific Sintered Materials FS-1603 Silicon Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC uses.All information provided by Pacific Sintered Metals. |
|||
Density | 7.00 g/cc | 0.253 lb/in³ | |
PSM Industries Ferro-TiC® CM-25 High Chrome Tool Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Ferr.. |
|||
Density | 7.00 - 7.20 g/cc | 0.253 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Iron Nickel FN-252-S Powdered Metal Very low coercive force and high permeability. Excellent for shielding and switching applications.Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 7.00 - 7.20 g/cc | 0.253 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Phosphorous Iron FP-1650-S Powdered Metal For applications requiring high yield strength and toughness. Magnetic properties superior to iron, but slightly inferior to silicon iron.Information Provided by Pacific Sintered Metals, a division .. |
|||
Density | 7.00 - 7.30 g/cc | 0.253 - 0.264 lb/in³ | |
PSM Industries Pacific Sintered Metals Silicon Iron FS-1603 Powdered Metal DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC usesInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | >= 7.00 g/cc | >= 0.253 lb/in³ | |
H.C. Starck Pure Molybdenum OMPP Pellets (99.8%) Description of Product: This specification covers vacuum grade pressed and sintered molybdenum pellets, with a molybdenum content of 99.8% minimum.Pellet Size: approx. 1/2 inch by 3/4 inch by 1 in.. |
|||
Density | >= 7.00 g/cc | >= 0.253 lb/in³ | |
H.C. Starck Pure Molybdenum WMPP Pellets (99.0%) Description of Product: This specification covers vacuum grade pressed and sintered molybdenum pellets, with a molybdenum content of 99.0% minimum.Pellet Size: approx. 1/2 inch by 3/4 inch by 1 in.. |
|||
Density | 7.00 g/cc | 0.253 lb/in³ | |
China Tungsten YT772-2 Titanium Carbide and Nitride Based Carbides Good wear resistance and better toughness, relative impact resistance , for intermittent turning and milling of cast iron and steel parts.Information provided by China Tungsten |
|||
Density | >= 7.00 g/cc | >= 0.253 lb/in³ | |
China Tungsten STG10-20 PM Structural Parts Information provided by China Tungsten |
|||
Density | 7.00 g/cc | 0.253 lb/in³ | |
PSM Industries Ferro-TiC® CHW-25 Hot Work Tool Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Ferr.. |
|||
Density | 7.00 - 7.20 g/cc | 0.253 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Invar FN-251-S Powdered Metal Coefficient of thermal expansion equal to glassInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 7.00 - 7.20 g/cc | 0.253 - 0.260 lb/in³ | |
PSM Industries Pacific Sintered Metals Iron F-241-S2 Powdered Metal DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores Equivalent ASTM Spec: B310-70, Type IV, Class AInformation Provided by Pacific Sintered Metals, a d.. |