Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.61 g/cc | 0.311 lb/in³ | |
Hoskins Manufacturing Alumel® Thermocouple Wire Type K - Std All values may vary dependent on specific design and usageAlumel® is a registered trade name of Hoskins Manufacturing.Capabilities: WireRibbonSquareInsulatedPlatedInformation provided by Californ.. |
|||
Density | 8.61 g/cc | 0.311 lb/in³ | Theoretical |
Kennametal Stellite Stellite® 31 PM cast Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous we.. |
|||
Density | 8.61 g/cc | 0.311 lb/in³ | Theoretical |
Kennametal Stellite Stellite® 31 PM with P/M Processing; heat treated at 93°C (200°F) and water quenched Typical applications include, miscellaneous wear parts. Data provided by the manufacturer, Deloro Stellite Inc.Product of former Deloro Stellite Inc. |
|||
Density | 8.60 g/cc | 0.311 lb/in³ | Sintered Typical |
Kinetics MIM Ni as Sintered Most commonly used for applications requiring: Electrical conductivity Corrosion resistance. Information provided by Kinetics, Inc. |
|||
Density | 8.60 g/cc | 0.311 lb/in³ | |
Indium Corp. Indalloy 73 Bismuth-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.60 g/cc | 0.311 lb/in³ | annealed |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Density | 8.60 g/cc | 0.311 lb/in³ | annealed |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Density | 8.60 g/cc | 0.311 lb/in³ | annealed |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Density | 8.60 g/cc | 0.311 lb/in³ | annealed |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Density | 8.60 g/cc | 0.311 lb/in³ | annealed |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Density | 8.60 g/cc | 0.311 lb/in³ | annealed |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Density | 8.60 g/cc | 0.311 lb/in³ | annealed |
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Density | 8.60 g/cc | 0.311 lb/in³ | annealed |
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Density | 8.60 g/cc | 0.311 lb/in³ | annealed |
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Density | 8.61 g/cc | 0.311 lb/in³ | |
Special Metals INCONEL® alloy 22 Austenitic Alloy INCONEL® alloy 22 (UNS N06022; W.Nr. 2.4602; NiCr21Mo14W) is a fully austenitic advanced corrosion-resistant alloy that offers resistance to both aqueous corrosion and attack at elevated temperat.. |
|||
Density | 8.62 g/cc | 0.311 lb/in³ | |
ATI Allegheny Ludlum AL 22™ Nickel-Base Alloy, UNS N06022 AL 22 alloy is a Ni-Cr-Mo alloy that provides outstanding resistance to pitting, crevice corrosion, intergranular attack, and stress corrosion cracking. The combination of Cr, Ni, Mo, and W provide.. |
|||
Density | 8.60 g/cc | 0.311 lb/in³ | annealed |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Density | 8.60 g/cc | 0.311 lb/in³ | annealed |
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Density | 8.61 g/cc | 0.311 lb/in³ | Theoretical |
Kennametal Stellite Stellite® 31 PM after P/M processing, aged 8 hours at 802°C air cooled Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous we.. |
|||
Density | 8.61 g/cc | 0.311 lb/in³ | Theoretical |
Kennametal Stellite Stellite® 31 PM cast aged 8 hours at 802°C air cooled Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous we.. |