Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.91 g/cc | 0.322 lb/in³ | |
Materion moldMAX® XL Spinodally Hardened Copper-Nickel-Tin Alloy moldMAX XL® is a unique spinodally hardened copper-nickel-tin alloy that combines high strength and high thermal conductivity. Available in large plate thickness up to 12†and in rounds up t.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
HP Alloys Alloy C-276, 40% Cold Worked 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
Goodfellow Nickel 70/Copper 30 Alloy Information provided by Goodfellow. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 110 EPT COPPER, 1/2 Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, 3/4 Hard 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Hard 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 194 HSM® Copper, 1/2 Hard High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 194 HSM® Copper, Extra Spring High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 194 HSM® Copper, Spring High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
Chicago Extruded Metals BioBrass® UNS C64700 Copper-Silicon Alloy Finished product available as bar, wire, or rod.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Meta.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
CLAL-MSX CUPROROR® TL5 Spring, Copper Alloy Alloy especially suited to applications in electronics and electro technology. This doped copper, displays high electrical and thermal conductivity, good mechanical properties and excellent temperat.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
CLAL-MSX NICLAFOR® 1000 TD1 Quenched/Cold Rolled, Rolled Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
CLAL-MSX NICLAFOR® 1000 TD4 Quenched/Cold Rolled, Rolled Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
CLAL-MSX NICLAFOR® 1000 TH3 Quenched/Precipitation Heat Treated, Drawn Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
CLAL-MSX NICLAFOR® 1000 TH4 Quenched/Precipitation Heat Treated, Drawn Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
CLAL-MSX NICLAL 3444 0 Annealed Copper Alloy, Free Cutting Bronze Main Characteristics: Excellent machineabilityHigh mechanical propertiesSelf lubricating alloyTypical Applications:Parts for connectorsFriction partsBearings-Pinions-Lock pinsInformation provided b.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
CLAL-MSX SICLANIC S® TD4 Quenched Copper Alloy, 4/4 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
CLAL-MSX SICLANIC S® TH4 Quenched Copper Alloy, 4/4 Hard, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
Cadi C11000 ETP Standard Grade Copper The standard grade of copper - most widely used electrical conductor - suitable where mechanical design is not an issue and maximization of electrical or thermal conductivity is the primary concern... |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
Ametek High Purity Nickel Strip 899A 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
Ametek High Purity Nickel Strip 899M Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
Ametek High Purity Nickel Strip 899M Skin Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
Ametek High Purity Nickel Strip 899G 50% Cold-Rolled Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
Ametek High Purity Nickel Strip 899G Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
Ametek High Purity Nickel Strip 899M 3/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Density | 8.90 g/cc | 0.322 lb/in³ | |
HP Alloys Alloy C-276, 30% Cold Worked 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |