Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.870 g/cc | 0.0314 lb/in³ | |
DuPont Fusabond® MN493D Ethylene Octene Copolymer
(discontinued **) Typical Use: Nylon 6 toughenerNylon 6/6 toughenerComplies to FDA 21CFR 175.105Availability: North AmericaInformation provided by DuPont. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | |
DuPont Fusabond® MN494D Ethylene Octene Copolymer
(discontinued **) Typical Use: Nylon 6 toughenerNylon 6/6 toughenerAvailability: North AmericaInformation provided by DuPont. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D1505 |
M. Holland Company MAGMA® LM372-A LLDPE
(discontinued **) Features: High Clarity, Good Flexibility, Good Flow, High Gloss, Good ToughnessProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | |
DuPont Fusabond® MF416D Ethylene Propylene Rubber
(discontinued **) Typical Use: Nylon 6/6 toughenerComplies to FDA 21CFR 175.105Availability: North AmericaInformation provided by DuPont. |
|||
Density | 0.870 - 0.930 g/cc | 0.0314 - 0.0336 lb/in³ | ASTM D 792 |
Karina 55/200-TR Kariprene Cristal Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Density | 0.870 - 0.930 g/cc | 0.0314 - 0.0336 lb/in³ | RP-1008 |
Solvay RHODOLINE® DF 540 Surfactant Description: Highly effective white oil defoamer for latex processing.Identification: DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© DF 540 is a general purpose silicone-free, high a.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D-792 |
Polyram BondyRam® 7001 Maleic Anhydride Modified Semi-crystalline EPDM Impact Modifier Maleic Anhydride Modified Semi-crystalline EPDM recommended as impact modifier for polyamide compounds.Information provided by Polyram Ram On Ind. |
|||
Density | 0.870 g/cc @Temperature 15.6 °C |
0.0314 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 1000 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Density | 0.870 g/cc @Temperature 15.0 °C |
0.0314 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Heavy Medium Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Density | 0.870 g/cc @Temperature 15.6 °C |
0.0314 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 220 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Density | 0.870 g/cc @Temperature 15.6 °C |
0.0314 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 460 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | |
DuPont™ Nomex® 410 Paper, 5 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Density | 0.870 g/cc @Temperature 15.6 °C |
0.0314 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 1000 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D792 |
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer AFFINITY™ EG 8200G Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. It exhibits high flexibility and elasticity. It can be utilized in monolayer cast film and in .. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | |
Dow AFFINITY™ SM 8400 Polyolefin Elastomer Data provided by Dow Chemical. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D792 |
Dow Engage® 8107 Polyolefin Elastomer Description: Engage® 8107 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D792 |
Dow Engage® 8200 Polyolefin Elastomer Description: Engage® 8200 and Engage® 8207 polyolefin elastomers are ethylene-octene copolymers that have excellent flow characteristics and performs well in a wide range of general purpose thermo.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D792 |
Dow Engage® 8207 Polyolefin Elastomer Description: Engage® 8207 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio.. |
|||
Density | 0.870 g/cc @Temperature 15.0 °C |
0.0314 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 80W-140 Synthetic Gear Oil Mobil Delvac Synthetic Gear Oil 75W-90 and 80W-140 are synthetic drivetrain lubricants engineered to meet the most demanding extended drain and warranty requirements. These products are designed for.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D297 |
Dow Nordel® IP 4760P EPDM Hydrocarbon Rubber Description: Nordel® IP 4760P is a semicrystalline, ethylenepropylene-diene (EPDM) terpolymer. The polymer's unique bimodal ethylene distribution provides a balance of processing characteristic.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D297 |
Dow Nordel® IP 4770P EPDM Hydrocarbon Rubber Description: Nordel® IP 4770P is a high molecular weight semicrystalline grade and offers fast cure rates and high states of cure with standard sulfur cure systems. It offers high green strength an.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | |
Dow AFFINITY™ EG 8200 Polyolefin Elastomer AFFINITY® EG 8200 polyolefin elastomer is a saturated ethylene-octene copolymer for general purpose elastomeric applications that is efficiently crosslinked by peroxide, silane or irradiation. It e.. |
|||
Density | 0.870 g/cc @Temperature 15.0 °C |
0.0314 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Heavy Medium Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | |
ConocoPhillips Hydroclear Diamond Class® 68 Turbine Oil Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | DIN 53479 |
ExxonMobil EXXELOR™ VA 1801 Maleic anhydride functionalized elastomeric ethylene copolymer Product Description: Exxelor VA 1801 polymer resin is a medium viscosity, semi-crystalline ethylene copolymer functionalized with maleic anhydride by reactive extrusion. Its fully saturated backbone.. |