Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | Average value: 0.903 g/cc Grade Count:89 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H13G-00 Polypropylene Homopolymer
(discontinued **) Formerly Amoco® 7444. Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Medical componentsComplies with FDA specification, Title 21, C.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Amoco® 7556 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: High speed spinning, Improved bulk, Low gas fadeTypical applications: Upholstery, BCF carpet yarnsComplies with FDA specification, Title 21, CF.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H00M-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, Enhanced flow, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical applications.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H03G-03 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: ExtrusionFeatures: Ease of processingTypical applications: Oriented filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Amoco® 7644 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Amoco® 7942 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Excellent mold release, AntistaticTypical applications: Closures, Thin-walled rigid packagingComplies with FDA specification, Title 21, CFR .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H38G-01 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: Very high speed spinning, Low gas fadeTypical applications: Spunbound fabricsComplies with FDA specification, Title 21, CFR 177.1520.Typical pr.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3119HS Ultra High Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High stiffness, Low Temperature impactComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3243 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3950 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Low gloss, High melt flow, Low temp impact, NucleatedComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below fro.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H03G-00 Polypropylene Homopolymer Suggested fabrication methods: ExtrusionFeatures: Low water carry-overTypical applications: Woven fabric, Cordage, Slit filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property d.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H05A-00 Polypropylene Homopolymer Grade H05A-00 is an antistatic polypropylene homopolymer for injection molding & extrusion applications. This material meeets the requirements of the U.S. Food and Drug Administration as specified .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H05M-00 Polypropylene Homopolymer Grade H05M-00 is a general purpose polypropylene homopolymer for injection molding applications. This resin provides good long-term heat stability. This material meets the requirements of the Food.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H13M-00 Polypropylene Homopolymer Grade H13M-00 is a general purpose polypropylene homopolymer for injection molding applications. It provides good long-term heat stability.Suggested fabrication methods: Injection moldingFeatures: .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H20H-00 Polypropylene Homopolymer This resin is designed to provide easy moldability for applications requiring resistance to long term heating. This material has been recognized by UL for sustained use at 130c.Suggested fabricatio.. |
|||
Density | 0.886 g/cc @Temperature 15.0 °C |
0.0320 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil Mobil Pegasus 801 40 Mobil Pegasus 801 is an SAE 40 premium performance gas engine oil intended for the lubrication of all classes of gas engines operating at low, medium and high speeds where low ash or ashless oils ar.. |
|||
Density | 0.886 g/cc | 0.0320 lb/in³ | |
ConocoPhillips Conoco® El Mar® 2000 Oil SAE Grade 40 Conoco® El Mar 2000 is a high-quality, very low-ash, dispersant detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged, low- to medium-speed 2-stroke cycle and.. |
|||
Density | 0.886 g/cc @Temperature 15.0 °C |
0.0320 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil Mobil Pegasus 801 40 Mobil Pegasus 801 is an SAE 40 premium performance gas engine oil intended for the lubrication of all classes of gas engines operating at low, medium and high speeds where low ash or ashless oils ar.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H05H-01 Polypropylene Homopolymer Grade H05H-01 is a homopolymer polypropylene for injection molding applications. It is an excellent long-term heat aging grade and offers superior extraction resistance in hot aqueous solutions. T.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Accpro® 9346 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Long-term heat aging, High stiffness, Nucleated, UL RecognizedComplies with FDA specification, Title 21, CFR 177.1520.Typical applications: .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Accpro® 9965 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: NucleatedTypical applications: CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H35Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3240 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Extrusion; Fiber Optic CableFeatures: NucleatedComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acclear® 8649X Random Copolymer Polypropylene, High Clarity Grade
(discontinued **) Developmental Grade. Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Low taste/odor, Excellent processabilityTypical applications: High clarity c.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acclear® 8939 Random Copolymer Polypropylene, High Clarity Grade
(discontinued **) Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Excellent static control, ToughenedTypical applications: Housewares, Rigid packaging, Media packag.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acclear® 8949 Random Copolymer Polypropylene, High Clarity Grade
(discontinued **) Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Excellent static controlTypical applications: Housewares, Thin-walled containers, Rigid packagingC.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H13Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical prope.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H35G-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520... |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3432 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples. |