Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.890 g/cc @Thickness 3.17 mm |
0.0322 lb/in³ @Thickness 0.125 in |
injection molded specimen; ISO 1133 |
Phillips Sumika Marlex® ABF-300 High Flow Thermoplastic Olefin
(discontinued **) Applications: Automotive exterior fasciasInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. |
|||
Density | 0.890 g/cc | 0.0322 lb/in³ | ISO 1183 |
LyondellBasell Adsylâ„¢ 5 C 37 F Polyolefin Description: Adsylâ„¢ 5 C 37 F is a new thermoplastic polyolefin which has been designed as a BOPP sealing layer material with exceptionally low sealing temperature. It features a high clarity an.. |
|||
Density | 0.890 g/cc | 0.0322 lb/in³ | ASTM D792 |
LyondellBasell Hifaxâ„¢ CA199AC Thermoplastic Olefin Resin Key Features: low melt flow, medium low modulus, paintable thermoplastic olefin resin, excellent balance of properties, high toughness, good paintability, flexibleApplications: automotive air bag do.. |
|||
Density | 0.890 g/cc | 0.0322 lb/in³ | ISO 1183 |
LyondellBasell Hifaxâ„¢ CA387 Thermoplastic Polyolefin Elastomer Description: Hifax â„¢ CA387 is a thermoplastic polyolefin elastomer suitable for automotive exterior partsFeatures: Good StiffnessGood ProcessabilityGood Impact ResistanceGood Colorability Paint.. |
|||
Density | 0.890 g/cc | 0.0322 lb/in³ | ISO 1183 |
LyondellBasell Hifaxâ„¢ CA45 Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus thermoplastic elastomeric olefin resin, excellent balance of properties, excellent processability, good colorability, excellent surface appearanceAppli.. |
|||
Density | 0.890 g/cc | 0.0322 lb/in³ | |
Stellarchem GP-975B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Density | 0.890 g/cc | 0.0322 lb/in³ | |
Silon Tabond 2002 Adhesive Resin TABOND 2002 is ethylene-octene Plastomer / LLDPE modified with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated glass.. |
|||
Density | 0.890 g/cc @Temperature 15.6 °C |
0.0322 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 680 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Density | 0.890 g/cc @Temperature 15.0 °C |
0.0322 lb/in³ @Temperature 59.0 °F |
|
ExxonMobil Kutwell 40 KUTWELL is the trademark for a line of two high-performance "soluble" cutting fluids for cooling and lubricating the tool and work in machining operations. The line includes one petroleum-base fluid.. |
|||
Density | 0.890 - 1.11 g/cc | 0.0322 - 0.0401 lb/in³ | |
Trelleborg Offshore Vikotherm™ 73585 Insulative Elastomer Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res.. |
|||
Density | 0.890 g/cc | 0.0322 lb/in³ | ASTM D 792 |
Cossa Polimeri ESTAPROP HK 4000 CH-HT Polypropylene Copolymer Polypropylene copolymer, high fluidityInformation provided by Cossa Polimeri S.r.l. |
|||
Density | >= 0.890 g/cc | >= 0.0322 lb/in³ | |
Elastron® G SEBS Elastomer Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureshigh temperature resistanceelectrical insulator with v.. |
|||
Density | 0.890 g/cc | 0.0322 lb/in³ | |
ExxonMobil Mytex™ AN17K-01 Rubber modified polypropylene for automotive interior applications.Information provided by ExxonMobil Chemical |
|||
Density | 0.890 g/cc @Temperature 15.0 °C |
0.0322 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 30 Mobiltrans HD Mobiltrans HD 10W, 30, 50, and 60 are extra high performance transmission and drive-train lubricants engineered to meet the rigorous specifications required by Caterpillar TO-4. This product line .. |
|||
Density | 0.890 g/cc @Temperature 15.6 °C |
0.0322 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 634 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Density | 0.890 g/cc @Temperature 15.6 °C |
0.0322 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil Spartan EP 100 Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin.. |
|||
Density | 0.890 g/cc @Temperature 15.6 °C |
0.0322 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil Spartan EP 68 Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin.. |
|||
Density | 0.890 g/cc | 0.0322 lb/in³ | ASTM D 792 |
Cossa Polimeri ESTAPROP KUR 4000 CH/TD Polypropylene Copolymer Polypropylene copolymer, elastomer modifiedInformation provided by Cossa Polimeri S.r.l. |