Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.916 - 0.920 g/cc | 0.0331 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4118Q (18403) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.916 - 0.920 g/cc | 0.0331 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 5117N (18601) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.916 - 0.920 g/cc | 0.0331 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 5117P (18602) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.916 - 0.920 g/cc | 0.0331 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 5118N (18601) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.916 - 0.920 g/cc | 0.0331 - 0.0332 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® CX 7065 LDPE - Extrusion Coating The Trithene® CX 7065 resin is a product developed especially to meet the segment of extrusion coating where the following properties are necessary: processing stability at high production rates, a.. |
|||
Density | 0.916 - 0.920 g/cc | 0.0331 - 0.0332 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® JX 7065 LDPE - Injection Molding and Master Batch The Trithene® JX 7065 resin is a low-density polyethylene with a wide molecular weight distribution, developed to offer good impact resistance, excellent flexibility, and high resistance to stress .. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | carrier resin value; ASTM D-1505 |
Chevron Phillips MarFlex® ER3341 Polyethylene; Masterbatch
(discontinued **) Metallocene polyethylene antiblock masterbatch. This antiblock concentrate with its mLLDPE carrier is tailored for use with mPACT™ resins in blown film applications that require: Reduced COFMinim.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | carrier resin value; ASTM D-1505 |
Chevron Phillips MarFlex® ER3343 Polyethylene; Masterbatch
(discontinued **) Metallocene polyethylene slip masterbatch. This erucamide slip concentrate with its mLLDPE carrier is tailored for use with mPact™ resins in blown film applications that require: Reduced COFExcel.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Chevron Phillips mPact™ D143SA m-LLDPE Linear Low Density Polyethylene
(discontinued **) Low Density PolyethyleneCustomer Benefits: This metallocene LLDPE film resin possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved proce.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Global ST-1018 Low Density Polyethylene, Injection Molding Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-packagingMeets FDA requirements as listed in food additives regulation 21 CFR 117.15.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Global SU-1018 Low Density Polyethylene, Injection Molding Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-packagingMeets FDA requirements as listed in food additives regulation 21 CFR 117.15.. |
|||
Density | 0.916 - 0.920 g/cc | 0.0331 - 0.0332 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4117P (18402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Huntsman PE5082 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings (sugar paper and laminations).FDA Notes: Con.. |
|||
Density | 0.916 - 0.938 g/cc | 0.0331 - 0.0339 lb/in³ | Average value: 0.920 g/cc Grade Count:84 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D792 |
LyondellBasell Montell 16501F4 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets F.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D792 |
LyondellBasell Montell 16501F8 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D792 |
LyondellBasell Montell 16502F7 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D1505-98 |
Ipiranga Petrochem LB 0216 LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D792 |
Micropol DD Polyethylene powders for cleaning products Information provided by Micropol Limited |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Micropol L7 Low density polyethylene rotational molding powder Has a high gloss finish, and outstanding toughness. Information provided by Micropol Limited |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ISO 1183 |
MTM Plastics Purpolen® PP Polypropylene Regrind Purpolen® is a sorted regrind material suited to the production of demanding end user products. Extrusion and injection molding grades are available in many colors. The basis of our Purpolen® .. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D1505 |
UBE J3519 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Westlake EM811AA Low Density Polyethylene WESTLAKE low-density polyethylene EM811 is a low-density polyethylene used for injection molding. It is characterized by high flow and low stiffness.Application/UsesFlexible medicalMedicalFDA: This .. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D792 |
Dow ELITE™ 5230G Enhanced Polyethylene Resin ™ 5230G is produced via INSITE™ Technology from Dow Plastics. It offers high impact strength and good puncture resistance at moderate stretch levels for irregularly shaped loads. In addition, th.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D792 |
Dow ELITE™ 5400G Enhanced Polyethylene Resin ™ 5400G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of low seal initiation, moderate stiffness and low blocking tendencies for good performanc.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | |
Dow LDPE 4005M Low Density Polyethylene Data provided by Dow Chemical. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | |
Dow LDPE 4012M Low Density Polyethylene DOW LDPE 4012M resin is a broad molecular weight distribution homopolymer designed to provide good impact strength, excellent flexibility and high stress crack resistance for housewares, toys and ge.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Braskem LH 118 LLDPE Blown Film Extrusion Polyethylene Description: LH118 is a Linear Low Density Polyethylene, copolymer of hexene-1, produced by Spherilene process. Developed for blown film extrusion in blends with polyethylenes. Films obtained with t.. |
|||
Density | 0.916 - 0.944 g/cc | 0.0331 - 0.0341 lb/in³ | Average value: 0.922 g/cc Grade Count:20 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Extrusion Grade". Each property range of values reported is min.. |
|||
Density | 0.916 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Braskem LL 118 LLDPE Blown Film Extrusion Polyethylene Description: LL118 is a Linear Low Density Polyethylene, copolymer of butene-1, produced by Spherilene process. Developed for blown film extrusion in blends with polyethylenes. Films obtained with t.. |