Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.923 - 0.926 g/cc | 0.0333 - 0.0335 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
SABIC HP4023W Low Density Polyethylene for Blown Film Product Description: HP4023W is a Low Density Polyethylene grade suitable for producing general purpose films and contains slip and antiblock additives. It yields excellent processability with goo.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Chevron Phillips 4522 LDPE Shrink and Heavy Duty Packaging Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Excellent Tensile Strength, Excellent Impact Strength, Very Good Tear Resistance, Very Good Abrasion Resistance, No Slip, No AntiblockApplications:Pallet Shri.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Chevron Phillips 5102 LDPE Injection Blow Molding Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Good Core Pin Release, Good Stability, Low Taste and Odor Characteristics, Good Impact and Toughness, Good Clarity on GlossApplications:Squeeze Bottles, Perso.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D792 |
DuPont Bynel® 11E573 Modified EVA Adhesive Resin
(discontinued **) Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
M. Holland Company EV200 EVA
(discontinued **) Features: Good Heat Seal, Opticals, High StrengthUses: PackagingApprovals: FDA 21 CFR 177.1350 and FDA 21 CFR 176.170,Table 2, Cond. C, D, E, F, GProcessing Method: Film, BlownInformation provided b.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
LyondellBasell Aquathene® AQ120000 Ethylene Vinylsilane Copolymer ApplicationsAQUATHENE AQ 120-000 is an ethylene vinylsilane copolymer designed for use in low voltage, power cable applications. This natural resin can be crosslinked, by exposure to moisture after.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® NA217000 Low Density Polyethylene ApplicationsPETROTHENE NA 217-000 is a high speed, lightweight coating resin for use with paper, films and other base stocks. This resin can yield coating weights down to 3.5 lbs/ream at line speed.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® NA217080 Low Density Polyethylene ApplicationsPETROTHENE NA 217-080 is a natural low density polyethylene resin formulated for use as primary insulation for coaxial and control cable applications. NA 217-080 has also been designed .. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Iran Petrochemical (PCC) 235F7 Linear Low Density Polyethylene 235F7 is a LLDPE blown film grade designed for general purpose film application. This resin is particularly suited for blending with LDPE, giving better strength and downgauging possibility.Informat.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ISO 1183 |
Borealis Bormed™ LE6603-PH LDPE for Healthcare Applications Bormed LE6603-PH is a low density polyethylene for injection molding having excellent flow properties allowing short cycle time or easy filling of long flow-paths. The molded article is characteriz.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ISO 1183 |
Borealis FT5232 Low Density Polyethylene FT5232 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes medium slip additive and antioxidant. This grade is developed for the production of packaging film with good op.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | LE 4421; ASTM D792 |
Borealis Visico™ LE4423/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4423/LE4432 is a black, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of a Visico base material.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | LE 4423; ASTM D792 |
Borealis Visico™ LE4423/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4423/LE4437 is a mature, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of a Visico base materia.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | LE 4423; ASTM D792 |
Borealis Visico™ LE4423/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4423/LE4460/LE4437 is a natural, halogen-based, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination o.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | Base LE 4423; ASTM D792 |
Borealis Visico™/Ambicat™ LE4423/LE4472 Black, Fast Curing, Silane Crosslinkable LDPE Compound for Weather Resistant Covering/Insulation of Overhead Cables Visico LE4423 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4472, will undergo an accelerated, moisture-induced crosslinking reaction. Th.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | LE 4421; ASTM D792 |
Borealis Visico™ LE4421/LE4460/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4421/LE4460/LE4432 is a black, halogen-based flame retardant, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 4517 LDPE Extrusion Coating Resin Resin Type: HomopolymerCharacteristics: Excellent Processability, Good MVTR, Good Heat Seal, Kosher ApprovedApplications:Liquid Packaging, Cup Stock, Folding Carton, General CoatingData provided by .. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | Base Density; ASTM D1505 |
Chevron Phillips MarFlex® 5428 LDPE Cast Film Resin Resin Type: HomopolymerCharacteristics: Excellent OpenabilitySuited for high speed convertingGood clarityLow COFApplications: Bakery FilmBreak BagsInformation provided by Chevron Phillips. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ExxonMobil Method |
ExxonMobil LD 124.MS General Purpose Clarity Film Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ExxonMobil Method |
ExxonMobil LD 302.20 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 101BA Wire & Cable Low Density Polyethylene Resin Product Description: LD 101BA Wire & Cable is anon-stabilized LDPE, designed for the production of Medium/High Voltage insulation using the direct peroxide addition. For cleanliness reasons, the mat.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 105.BR Low Density Polyethylene Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 124.MS Low Density Polyethylene Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 143.26 Low Density Polyethylene Resin Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | |
Dow LDPE 133A Low Density Polyethylene, Blown Film Grade DOW LDPE 133A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of antib.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | |
Dow LDPE 779I Low Density Polyethylene DOW LDPE 779I resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent rigidity. Typical applications include caps.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | |
Dow LDPE 959I Low Density Polyethylene DOW LDPE 959I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility with low warpage for lids. This resin has good processability over a wi.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ISO 1183 |
Fainplast Compounds Ethylplus 600 Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesSolid LDPEInformation provided by Fainplast Compounds.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | |
Dow LDPE 5004I Low Density Polyethylene, Extrusion Coating Grade DOW Polyethylene 5004I extrusion coating resin is a low melt index resin for heavy duty applications such as paperboard coatings, milk cartons and folding cartons, aseptic package coatings, bag line.. |