Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.921 - 0.925 g/cc | 0.0333 - 0.0334 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4223T (23407) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.921 - 0.925 g/cc | 0.0333 - 0.0334 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4223V (23416) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.922 - 0.925 g/cc | 0.0333 - 0.0334 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TS 7045 LDPE - Film - Plastification The Trithene TS 7045 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 107-276 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 107-277 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 107-278 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 107-279 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 108-276 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 108-277 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 158-280 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 158-281 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 162-280 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 162-281 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 108-278 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 108-279 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.919 - 0.925 g/cc | 0.0332 - 0.0334 lb/in³ | BRCP 4843 |
ExxonMobil Jayflex™ DINA Plasticizer Appearance: Clear and FreeAvailability: North AmericaCAS Number: 33703-08-01Information provided by ExxonMobil |
|||
Density | 0.916 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | Average value: 0.920 g/cc Grade Count:34 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum.. |
|||
Density | 0.922 - 0.925 g/cc | 0.0333 - 0.0334 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |