Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.926 - 0.930 g/cc | 0.0335 - 0.0336 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4028X (28435) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D4883 |
ExxonMobil LL 6202 Injection Molding Resin
(discontinued **) LL 6202 is a narrow molecular weight butene copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that require outstanding tear.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D4883 |
Eastman M30036-P Polyethylene
(discontinued **) M30036-P is an extrusion coating performance polymer suggested for applications requiring performance similar to LLDPE. Compared to low density coating resins, M30036-P offers superior heat seal st.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D792 |
DuPont Bynel® E326 Acid-/Acrylate-Modified EVA Adhesive Resin
(discontinued **) Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-307 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer, clarity film resin. Film made from this resin has superior impact strength and heat sealability.Applications: Froze.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D1505 |
Huntsman PE1503 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D1505 |
LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade ApplicationsMicrothene MP574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items. MP574189 is 16 mesh pow.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® GA574189 Linear Low Density Polyethylene, Injection Molding Grade PETROTHENE GA574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items.Regulatory Status: GA574189 meets th.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® NA420000 Low Density Polyethylene ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5074 800 Micron LLDPE Powder Description: ICOFLO 510-5074 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D1505 |
Lushan RF1000 Adhesive Resin for Aluminum Plastic Composite Pipe Adhesive resin Lushan series for aluminum-plastic composite pipe is maleic grafted polyethylene used for PE-AL-PE, PEX-AL-PEX and PERT-AL-PERT composite pipes. Lushan adhesive resin could provides i.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D792 |
DuPont Bynel® 4125 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D1505 |
Westlake Hifor Clear SC74580 Linear Low Density Polyethylene WESTLAKE Hifor Clear Polyethylene SC74580 polymer is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock. It doe.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 5755 LDPE High Clarity, High Impact Film Resin Resin Type: HomopolymerCharacteristics: High Clarity, Excellent Impact Strength, Medium Slip, High Antiblock, Moderately High Coefficient of Friction, Excellent ProcessabilityApplications:Case Shrin.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ExxonMobil Method |
ExxonMobil LD331.99 EVA LD 331.99 Very Clear, High Impact Film Resin LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 331.08 Low Density Polyethylene Resin Product Description: LD 331.08 is a 5.9% vinyl acetate copolymer, higher clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Availability: Latin Amer.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 361JD Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D4883 |
ExxonMobil LL 6201.19 Injection Molding Resin Product Description: LL 6201 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that req.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 6201XR Molding Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6201 series are high flow LLDPE grades, which offer unique combination of excellent processability and outstanding product properties. Parts manufactured from LL 6201 Have go.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 6201XR Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6201 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: N.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D792 |
Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-7147 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as food containers, housewares and lids. Information provided by D.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D792 |
Dow DNDA-8335 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8335 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | |
Dow DOWLEX™ 2505 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2505 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with good rigidity. It has ex.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | |
Dow Elite® 5110 Linear Low Density Polyethylene 5110 enhanced polyethylene resin is a copolymer produced via INSITE Technology from Dow Plastics. It offers unique combination of high modulus and excellent impact strength, allowing for downgaugin.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM-D1505 |
Braskem ML2400N LLDPE Injection Molding Polyethylene The resin ML2400N is a linear low-density polyethylene, 1-butene based, with good flexibility and low warpage. It does not contain a slip agent. It does have narrow molecular weight distribution. Th.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D792, ISO 1183 |
DuPont Elvax® PE3507-2 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® PE3507-2 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Applic.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-316 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 1.9% vinyl acetate copolymer, high clarity film resin. Film made from LD-316 offers improved impact strength and heat sealability versus homopoly.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-331 EVA Film Resin, Very High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® L62608PA Film (Hexene Grade) LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he.. |
|||
Density | 0.926 g/cc | 0.0335 lb/in³ | |
Dow LDPE 535I Low Density Polyethylene, Liner Grade DOW LDPE 535I resin is a barefoot general purpose liner resin with medium clarity for medium modulus packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for.. |