Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM D 792 |
NOVA Chemicals Surpass® IFs932-R Octene SLLDPE Injection Molding Resin IFs932-R complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM D792 |
Rochling Engineered Plastics Polystone® XL Cross linked (UHMW-PE) Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the .. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-701 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt, 10.5% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughnes.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | |
LyondellBasell Lupolen® 3220 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | |
LyondellBasell Lupolen® 3226 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM D792 |
LyondellBasell Hifaxâ„¢ AA56H Polypropylene Homopolymer Description: Hifaxâ„¢ AA56H medium high melt flow, 1,400 MPa flexural modulus, UL 94 V-2 flame retardant polypropylene homopolymer resin has an excellent combination of properties and processabil.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP FX04491H PE LNP LUBRICOMP* FX04491H is a compound based on Polyethylene resin containing Proprietary Fillers. Added features of this material include: Wear Resistant. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Catalyst CT/2 Polyolefin Catalyst CT/2 is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Cogegum® GFR series compounds, it all.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Catalyst CT/2-LR Polyolefin Catalyst CT/2-LR is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Cogegum® GFR series compounds, it .. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM-D1505 |
Westlake DA502AA 12% EVA Copolymer (Experimental Product) Westlake DA502AA is a 12% EVA copolymer designed for blown film applications. AA formulation contains no slip and no antiblock. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | with antiblock; ASTM D1505 |
Westlake Elevate™ EF563 6.5% Ethylene Vinyl Acetate Copolymer Westlake EF 563 resin is a fractional melt index 6.5% EVA copolymer with excellent drawdown, low melting/dispersion, and clarity optics in a soft but very tough film. Kosher compliant.Application/U.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 701.ID Blown Film Resin Escorene Ultra LD 701.ID is a fraction melt index, 10.5 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particularly.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ExxonMobil method |
ExxonMobil Escor™ 6000 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 6000 is primarily intended for extrusion coating and coextrusion coating. Escor 6000 is the high draw down version of Escor 5000. Very low coating weight achievable at hig.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Appeel® 72D799 Sealing Resin DuPont™ Appeel® 72D799 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 8360.29 Linear Low Density Polyethylene Resin Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM D4883 |
ExxonMobil LLP8360.29 Rotational Molding Resin Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ISO 1183 |
Fainplast Compounds Ethylplus 615 MD Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesSolid MDPEInformation provided by Fainplast Compounds.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | |
Dow Primacor® 3340 Ethylene Acrylic Acid (EAA) PRIMACOR® 3340 polymer containing 6.5% comonomer is an extrusion/ coextrusion coating and laminating for flexible packaging applications. It is designed to provide excellent adhesion and outstandin.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM D792 |
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM D792 |
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM-D792 |
Braskem FP33 LLDPE Blown Film Extrusion Polyethylene Copolymer The FP33 resin is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process for film extrusion with good mechanical properties. It contains processing aid, slip, and.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | Melt; ISO 1183 |
BASF Ultramid® 8202 HS PA6 (Conditioned) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | Melt; ISO 1183 |
BASF Ultramid® 8202 PA6 (Conditioned) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | Melt; ISO 1183 |
BASF Ultramid® 8202 PA6 (Dry) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | ASTM D1505 |
Arkema Group OREVAC® 9309 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Density | 0.932 - 1.64 g/cc | 0.0337 - 0.0592 lb/in³ | Average value: 1.19 g/cc Grade Count:114 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-8302 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8302 is the base re.. |
|||
Density | 0.932 g/cc | 0.0337 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-8361 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8361 is fully formu.. |