Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.933 - 0.937 g/cc | 0.0337 - 0.0339 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4435S (35405) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.933 - 0.937 g/cc | 0.0337 - 0.0339 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4436S (35405) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Tritheva® TN 2007 EVA Copolymer The Tritheva TN 2007 resin is an Ethylene-Vinyl Acetate copolymer (EVA), developed to meet the multi-layer packaging needs where are required high strength, with high toughness, and excellent optica.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® GA594189 Linear Low Density Polyethylene, Injection Molding Grade PETROTHENE GA594189 is a pelletized LLDPE copolymer resin for injection molding thin-walled items requiring high flow and short cycle times. GA594189 exhibits excellent flow, warp resistance and sur.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® GA694189 Linear Low Density Polyethylene, Injection Molding Grade PETROTHENE GA694189 is a pelletized LLDPE copolymer resin for injection molding. Typical applications include lids and thin-walled items that require high flow and short cycle times. GA694189 exhibi.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ASTM D1505-98 |
Ipiranga Petrochem MB 0435 MDPE IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) MF3313 High Density Polyethylene MF3313 is a high molecular weight high density polyethylene . Applications: extrusion, film, blown, bags, and density modifies.Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | LE 4437; ASTM D792 |
Borealis Visico™ LE4481/LE4437 Moisture-Crosslinking Polyethylene Compound for Flexible Low Voltage Insulation Visico LE4481/LE4437 is a natural, low-density ethylene vinyl silane/ ethylene butyl acrylate terapolymer that is designed for flexible low voltage wire insulation and jacketing. The combination of.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ASTM D1505 |
UBE Z322 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ISO 1183/ISO 1872-2 |
Borealis Visico™/Ambicat™ LE4421/LE4472 Polyethylene Compound, Crosslinkable Visico™ LE4421 / Ambicat™ LE4472 is a silane crosslinkable black compound designed for covering/insulation of overhead cables. The base material Visico™ LE4421 in combination with the catalyst m.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | Catalyst LE 4476; ASTM D792 |
Borealis Visico™/Ambicat™ ME4425/LE4476 Ambient Curing, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation Visico LE4423 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4476, will undergo an accelerated, moisture-induced crosslinking reaction. Th.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ASTM D792-ISO 1183 |
DuPont Elvax® 670 Ethylene Vinyl Acetate DuPont™ Elvax® 670 is an ethylene-vinyl acetate copolymer resin for use in industrial applications.Applications:Elvax® 670 resins can be used for the following applications: molding, compounding .. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ASTM D792 |
DuPont Elvax® 670 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | D1505 |
Westlake EF522 12% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF522 is an ethylene vinyl acetate copolymer with 12% VA. EF522 is designed for blown and
cast films requiring excellent optics and low heat seal initiation. High melt strength m.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® D350 m-LLDPE Linear Low Density Polyethylene Low Density PolyethyleneCustomer Benefits: This medium density metallocene polyethylene film resins combines the benefits of .933 density (modulus, barrier, c.o.f.) with the clarity of mLLDPE.Applic.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 713.93 Cast Film Resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer film resin. Film made from LD 713.93 exhbits very high impact strength, hihg clarity, and excellent heat sealabilityAvailability: Latin.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 713.93 Molding, extrusion and compounding resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer with very good toughness, high clarity and excellent processability. It is suitable for use in making molded articles, extruded profile.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® UL 7510 Adhesive Application Resin Escorene Ultra UL 7510 is a very high flow, 18.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, s.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ FL 00212 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00212 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 260°C (500°F) may cause resin degradation. Machines should always b.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ExxonMobil method |
ExxonMobil Escor™ 5020 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5020 is primarily intended for extrusion coating and coextrusion coating. Very good adhesion to polar substrates, aluminum foil, metalized films, papers, iron, steel and g.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 152BW Low Density Polyethylene Resin Product Description: LD 152BW is an LDPE grade offering an excellent combination of optical properties and stiffness. The 2.2 MI makes it ideal for blowing thicker films.Availability: Africa & Middl.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ASTM D792 |
Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-1082 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | ISO 1183 |
Fainplast Compounds Ethylplus 619 LD Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesBlack LDPE SheathingInformation provided by Fainplast.. |
|||
Density | 0.933 - 1.27 g/cc | 0.0337 - 0.0459 lb/in³ | Average value: 0.958 g/cc Grade Count:129 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | Catalyst LE 4476; ASTM D792 |
Borealis Visico™/Ambicat™ LE4423/LE4476 Fast Curing, Easy Processing, Environmentally Friendly, Silane Crosslinkable LDPE Compound for Low Voltage Insulation Visico LE4423 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4472, will undergo an accelerated, moisture-induced crosslinking reaction. Th.. |
|||
Density | 0.933 g/cc | 0.0337 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-713 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 15% vinyl acetate copolymer film resin. Film made from LD-713 exhibits very high impact strength, high clarity and excellent heat sealability.App.. |