Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.940 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792-91
Multibase Multi-Flex® TPO D-6509
Multi-Flex® A-6509 thermoplastic elastomer blend is designed to provide processors with cost effective compounds with excellent tear strength, tensile strength and high elongation. Multi-Flex® A-..
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Multibase Multi-Pro® 0612 CW Polypropylene
Calcium carbonate filler, 6% filer by weightForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Density 0.940 g/cc
0.0340 lb/in³
ISO 1183-A
Okulen® 1000 - REG PE Colored
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Density 0.940 g/cc
0.0340 lb/in³
Premix Thermoplastics PREADD UV 115
PREADD UV 115 is a masterbatch giving very good UV protection to polyolefin plastics. The active ingredient consists of HALS (Hindered Amine Light Stabilizer), which gives the most effective light s..
Density 0.940 g/cc
0.0340 lb/in³
Finaprene 2602 Test
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel..
Density 0.940 - 5.30 g/cc
0.0340 - 0.191 lb/in³
Average value: 2.75 g/cc Grade Count:96
Overview of materials for Epoxy, Electrically Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of..
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
DuPont™ Surlyn® 8120 Ionomer Resin, Sodium  (discontinued **)
Surlyn® 8120 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
DuPont™ Surlyn® 8527 Ionomer Resin, Sodium  (discontinued **)
Surlyn® 8527 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Density 0.940 g/cc
0.0340 lb/in³
ASTM D1505
ICO Polymers ICORENEâ„¢ 155-1326 LMDPE Rotational Molding Resin
Description: ICORENE 155-1326 is a linear medium density polyethylene developed for use in rotational molding. It has a great combination of stiffness and toughness in a resin that is easy processi..
Density 0.940 g/cc
0.0340 lb/in³
ASTM D1505
Lushan VB517 Adhesive Resin for Aluminum-Plastic Composite Panel (ACP), High Temperature
Adhesive resin Lushan series for Aluminum-plastic Composite Panel (ACP) proved required bonding strength between aluminum and the filled polyethylene core. The sandwich structure of Aluminum-plastic..
Density 0.940 g/cc
0.0340 lb/in³
MBA Method
MBA Polymers HDPE 1107 E Post-consumer recycled fractional melt high density polyethylene
Available in standard black.Information provided by MBA Polymers.
Density 0.940 g/cc
0.0340 lb/in³
Base Resin; ASTM D1505
Borealis Borecene Compact™ RM8406 Black Linear Polyethylene for Rotational Molding
Borecene Compact RM8406 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides ..
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
DuPont Elvax® 3170SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.Elvax® 3170SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res..
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792 - ISO 1183
DuPont Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer
Elvaloy® 1218 AC is intended for coextrusion, compounding and injection molding. Elvaloy® 1218 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent sealing pro..
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
DuPont Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin
Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Density 0.940 g/cc
0.0340 lb/in³
ISO 1183
Topas Advanced Polymers TOPAS® Elastomer E-140 Developmental Cyclic Olefin Copolymer (COC)
TOPAS® Elastomer E-140, unlike most TOPAS grades, is a semicrystalline cyclic olefin material with flexibility. It is a fairly stiff elastomer which can be extruded and injection molded, and can be..
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792, ISO 1183
DuPont™ Appeel® 72D727 Sealing Resin
DuPont™ Appeel® 72D727 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP..
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792, ISO 1183
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792, ISO 1183
DuPont™ Surlyn® 8528 Sodium Ionomer
Surlyn® 8528 is a sodium ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 8528 thermoplastic resi..
Density 0.940 g/cc

@Temperature 23.0 °C
0.0340 lb/in³

@Temperature 73.4 °F
ISO 1183
Arkema Group LOTRYL® 24 MA 005 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 24 MA 005 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 24 MA 005 is a poly..
Density 0.940 g/cc
0.0340 lb/in³
ASTM-D1505 / ASTM-D792
Braskem Evateno® 3019 PE EVA Foam Copolymer
Evateno® 3019 PE is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium vinyl-acetate content. Evateno® 3019 PE is an easy processing and crosslinkable product with high compatibility with oth..
Density 0.940 g/cc
0.0340 lb/in³
ASTM-D1505
Braskem PN2021 EVA Foam Copolymer
PN2021 is an Ethylene-Vinyl Acetate (EVA) copolymer mainly used for the production of crosslinked/expanded plates and other parts. It is a product with easy processability and high compatibility wit..
Density 0.940 g/cc
0.0340 lb/in³
ISO 2781
Alliance Polymers Viprene™ G40D-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G40D-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Density 0.940 g/cc

@Temperature 23.0 °C
0.0340 lb/in³

@Temperature 73.4 °F
ISO 1183
Arkema Group BONDINE® HX 8290 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
BONDINE® HX 8290 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. This grade is characterised by a high fluidity. Due..
Density 0.940 g/cc

@Temperature 23.0 °C
0.0340 lb/in³

@Temperature 73.4 °F
ISO 1183
Arkema Group LOTADER® 3410 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 3410 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 3410 is a versatile adhesive for extrusion coating or lam..
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792, ISO 1183
DuPont™ Fusabond® M603 Polymer Modifier
Fusabond® M603 Resin is a random ethylene copolymer, incorporating a monomer which is classified as being a maleic anhydride equivalent for application uses.Fusabond® M603 is used in a variety of ..
Density 0.940 g/cc
0.0340 lb/in³
BASF Myristyl Chloroformate
Formula: C15H29ClO2CAS: 56677-60-2Description: Myristyl Chloroformate is a colorless to yellowish liquid with a pungent odor. Synonyms: Chloroformic acid tetradecyl ester, Carbonochloridic acid, tet..
Density 0.940 g/cc
0.0340 lb/in³
Exxon Method
ExxonMobil Escorene® LD-734 High EVA Extrusion Coating Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and..
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Teknor Apex Sarlink® 4149D Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4149D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re..
Density 0.940 g/cc
0.0340 lb/in³
ISO 1183
Unipetrol PE HD LITEN® ZB 20 HDPE
Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA
Copyright © lookpolymers.com All Rights Reserved