Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Polymer Industries Densetec HDPE Pipe Grade The material displays improved performance characteristics in a variety of piping applications. In addition the material is UV stabilized and ideal for use in demanding outdoor applications. It reta.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | Compression Molded; ASTM D792 |
NOVA Chemicals Surpass® RMs244-UG Octene sHDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Standards 1.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D792 |
DuPont Nucrel® 2806 Ethylene-Acrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2806 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® HHM TR-480X HDPE Pipe and Corrugated Extrusion Resin
(discontinued **) Characteristics: Good long-term hoop strength performanceVery high melt strengthOutstanding low temperature toughnessApplications: Municipal, industrial, and mining pipeOil and gas gathering pipeInf.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | Compression Molded; ASTM D792 |
NOVA Chemicals Surpass® RMs244-U Octene sHDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Standards 1.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | Natural; ASTM D4883 |
Ineos K44-15-186 Polyethylene Copolymer K44-15-186 is a blue high-density polyethylene copolymer designed specifically for extrusion of pipe by blending K44-15-122 natural resin with G38-70C BLU II concentrate or an approved equivalent. .. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D4883 |
Ineos K44-24-122 HDPE K44-24-122 is a high density polyethylene copolymer designed specifically for pipe coating and extrusion. It complies with the virgin polyethylene resin requirements in CZA Z245-21.Natural resin; s.. |
|||
Density | 0.944 - 0.948 g/cc | 0.0341 - 0.0342 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GD 5150 K HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.944 - 0.948 g/cc | 0.0341 - 0.0342 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GM 9245 F HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.944 - 0.950 g/cc | 0.0341 - 0.0343 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem HD 7555 LS-L HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) BL8 HM 7745 High Density Polyethylene BL8 (HM 7745) is a high density polyethylene with Butene-1 as comonomer.Applications: for heating oil storage tanks, large containers for various chemicals.Information provided by Iran Petrochemical.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) EX 6HT HM 9455 HT High Density Polyethylene EX 6HT is a high density polyethylene with 1-Butene as co monomer. It has good toughness, low gel level, good tear strength, high tenacity.Applications: film extrusion, blending partner, refuse ba.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D792 |
Micropol Isoplas P381 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D4883 |
Ineos K44-06-122 HDPE HDPE K44-06-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as .. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Polidan® T/A-HF Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-HF is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | DIN 53479/ASTM D1505 |
Silon Taborex TA 1132 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1132 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | Base Resin; ISO 1183 |
Borealis BorPEX™ HE2595 Black High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation)) BorPEX HE2595 is a black, molecular weight, high density polyethylene compound for crosslinkable pipes, especially designed for electron beam irradiation crosslinking. The stabilization package is .. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | Natural; ASTM D1505 |
Formosa Plastics Formolene® HP4401 Pipe HDPE High Density Hexene CopolymerApplications: Potable water, industrial mining, oil and gas gatheringsFormolene HP4401 is a high performance copolymer that is designed for the most demanding requiremen.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | masterbatch; ASTM D-1505 |
Chevron Phillips Marlex® M368 Polyethylene; Masterbatch This black masterbatch with its medium density polyethylene (MDPE) carrier resin has been formulated for pipe applications that require: Good long-term hoop strengthExtended outdoor lifeClean N550 .. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ExxonMobil method |
ExxonMobil Escor™ 5200 Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5200 is an ethylene acrylic acid copolymer with a high comonomer content. Escore 5200 can be used pure or as a component in blend formulations for bonding applications whe.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Elvaloy® AC 12024S Ethylene Methyl Acrylate Elvaloy® AC 12024S is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy®.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Elvaloy® AC 15024S Ethylene Methyl Acrylate Elvaloy® AC 15024S is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy®.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM-D792 |
Braskem GM7746C HDPE Blow Molding Polyethylene GM7746C is a high-density polyethylene specially developed for the manufacturing of blow molding fuel tanks. It has high molar mass and excellent mechanical properties. It also shows excellent tenac.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM-D792 |
Braskem GM7746CA HDPE Blow Molding Polyethylene GM7746CA is a high-density polyethylene specially developed for the manufacturing of blow molding fuel tanks. It has high molar mass and excellent mechanical properties. It also shows excellent tena.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | Base Resin; ISO 1183 |
Borealis BorPEX™ HE2591 High Density Polyethylene Powder for Crosslinked Pipes (Pex-C (Irradiation)) BorPEX HE2591 is a high molecular weight, high density polyethylene powder for crosslinkable pipes, offering excellent processability for peroxide crosslinking. It is a special polymer, stabilized .. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HP4000 Pipe HDPE High Density Hexene Copolymer Formolene® HP4000 is a high performance copolymer that is designed for the most demanding requirements of non pressure pipe applications. It has good long-term hoop st.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D1505 |
Westlake EMAC® SP 1257 Ethylene-Methyl Acrylate Copolymer
(discontinued **) 20% Methyl Acrylate Content. Characteristics: FDA Clearance for Packaging of Most Foods, Including Aseptic Packaging; Less Crystalline and Softer than Polyethylene; Excellent Heat Stability Allows .. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D792 |
LyondellBasell Alathon® L4434 High Density Polyethylene ApplicationsALATHON L 4434 is a medium molecular weight high density copolymer for use in blown film applications. Typical applications include blown film over pouches. Regulatory StatusL 4434 meet.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | ASTM D792 - ISO 1183 |
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1126 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Density | 0.944 g/cc | 0.0341 lb/in³ | Base Density; ASTM D1505 |
Chevron Phillips Marlex® M362 LLDPE Pipe and Corrugated Extrusion Resin
(discontinued **) Characteristics: Good long-term hoop strengthExtended outdoor lifeClean N550 carbon blackApplications: PipesNot recommended for contact with food productsInformation provided by Chevron Phillips. |