Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.949 - 0.953 g/cc | 0.0343 - 0.0344 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6751E (516H5) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.949 - 0.953 g/cc | 0.0343 - 0.0344 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6752E (516H5) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.928 - 0.953 g/cc | 0.0335 - 0.0344 lb/in³ | Average value: 0.940 g/cc Grade Count:22 |
Overview of materials for EMAAA Terpolymer This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Density | 0.947 - 0.953 g/cc | 0.0342 - 0.0344 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem HE 7250 LS-L HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.947 - 0.953 g/cc | 0.0342 - 0.0344 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GF 5150 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |