Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D1505 |
Network Polymers NPP 50-0158 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Density | 0.958 - 0.962 g/cc | 0.0346 - 0.0348 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 2060S (60105) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.958 - 0.962 g/cc | 0.0346 - 0.0348 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 2060V (60118) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.958 - 0.962 g/cc | 0.0346 - 0.0348 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 2260M (601F7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 19C Homopolymer HDPE Film Resin Film Properties. Features: Good stiffness, good barrier, high clarity, narrow MWD.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D 792 |
Total Finathene® 3407B Black HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Density | 0.958 - 0.964 g/cc | 0.0346 - 0.0348 lb/in³ | |
Kazanorgsintez 294-73 High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: Composition of HD grad.. |
|||
Density | 0.958 - 0.963 g/cc | 0.0346 - 0.0348 lb/in³ | |
Kazanorgsintez 295-73 High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: Composition of HD grad.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L5840 High Density Polyethylene ApplicationsALATHON L 5840 is a lightweight resin that exhibits excellent color, low odor and provides processing stability. Typical applications include household chemicals, industrial chemicals, .. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® L5845 High Density Polyethylene ApplicationsALATHON L 5845 is a medium molecular weight high density homopolymer for use in blown film applications. Typical applications include paper replacement, coextrusions and laminations.Reg.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® M6028 High Density Polyethylene ApplicationsM 6028 is a homopolymer that is warp resistant, exhibits excellent toughness, stiffness and color as well as low odor and good processing stability. Typical applications include safety .. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D1505 |
Global J-1600 High Density Polyethylene Description-suitable for injection moldingApplications-household products, handy craft flowers, toys, stationaryInformation provided by Global Polymers Corporation. |
|||
Density | 0.958 - 0.964 g/cc | 0.0346 - 0.0348 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GF 4960 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.958 - 0.962 g/cc | 0.0346 - 0.0348 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GM 8260 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D792 |
LyondellBasell Alathon® L5885 High Density Polyethylene ApplicationsALATHON L 5885 is a medium molecular weight high density homopolymer for use in blown film applications. Typical applications include those low WVTR requirements.Regulatory StatusL 5855.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D1505 |
Iran Petrochemical (PCC) 60507 High Density Polyethylene 60507 is a HDPE injection molding grade which combines good flowability with balanced physical properties. This resin is well suited for general purpose applications requiring high stiffness. Applic.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Polidan® S/I 20 Polyethylene, Crosslinked (XLPE) POLIDAN® S/I 20 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for injection molding.Features: Crossl.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | |
Silon Tabond 3043 Adhesive Resin TABOND 3043 is HDPE modified with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated glass.Characteristics: • Stro.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | Compound; ISO 1183 |
Borealis BorPEX™ HE2557 Yellow High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide)) BorPEX HE2557 is a yellow, high molecular weight, high density polyethylene compound for crosslinkable pipes, specially designed for peroxide crosslinking. Long term stability and UV resistance is .. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ISO 1183 |
Borealis BS2581 High Density Polyethylene for Blow Molding BS2581 is a high density polyethylene intended for blow molding products with high stiffness and very good environmental stress crack resistance (ESCR). Applications: industrial chemicals, househol.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ISO 1183 |
Borealis FL5580 High Density Polyethylene FL5580 is a high density polyethylene with an excellent combination of extrusion properties and moisture barrier properties. Applications: FL5580 has been developed especially for applications like.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ISO 1183/ISO 1872-2 |
Borealis VL4580 High Density Polyethylene VL4580 is a high density polyethylene. This grade is especially designed for monofilament production. Applications: ropes, twines, nets, straps and brushes.Information provided by Borealis AG |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D792 |
Total 9458 HDPE Film Grade Medium molecular weight grade. Excellent bubble stability, good compatibility with LDPE and LLDPE, good heat resistance, high stiffness and tensile strength.Applications: Release liners, Stand-up ba.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D792 |
Total HDPE B5845 High Density Polyethylene - Blow Molding Resin Bimodal HDPE Blow Molding ResinCharacteristics:Excellent stress cracking resistanceExcellent stiffnessApplications:Household chemicalsIndustrial chemicalsIndustrial partsFood packagingPersonal care .. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ExxonMobil method |
ExxonMobil HDPE HD 7845.30 High Density Polyethylene Resin Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides exc.. |
|||
Density | 0.958 - 0.964 g/cc | 0.0346 - 0.0348 lb/in³ | BRCP 4843 |
ExxonMobil Jayflex™ L911P Plasticizer Appearance: Clear and FreeAvailability: North AmericaCAS Number: 685151-43-5Information provided by ExxonMobil |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM-D792 |
Braskem IB58 HDPE Injection Molding Polyethylene Copolymer IB58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers good processability combined with good .. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® HB-W558-A HDPE Extrusion Resin
(discontinued **) Molded Plaque Properties. Features: High molecular weight, excellent impact strength, high rigidity, easy processing.Applications: large part blow molding, large oil drums.Data provided by the manu.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | Exxon Method |
ExxonMobil Escorene® HDZ-128 MMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.Can be processed on high stalk, pocket extrusion or cast lines. Films made from HDZ-128 exhibit an excellent stiffness balance. High thermal stabi.. |
|||
Density | 0.958 g/cc | 0.0346 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® 9301 High Density Polyethylene ApplicationsALATHON 9301is a high density resin designed for sheet extrusion and thermoforming. It exhibits very low sag and high stiffness.Regulatory StatusALATHON 9301 meets the requirements of F.. |