Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.950 - 1.00 g/cc @Temperature 20.0 °C |
0.0343 - 0.0361 lb/in³ @Temperature 68.0 °F |
|
Hong Kun Group AO 1135 Antioxidant This product is phenols antioxidant, applicable to the occasion that there are liquor, latex, soliquoid and mixture,especially applicable to polyols and polyurethane.it has excellent effect in anti-.. |
|||
Density | 0.900 - 1.00 g/cc @Temperature 20.0 °C |
0.0325 - 0.0361 lb/in³ @Temperature 68.0 °F |
Grade A |
Kazanorgsintez Polyalkylbenzene Resin Production Method: Polyalkylbenzene resin is the by-product of isopropyl benzene production. Application: Intended for national economic needs and Grade A is exportedInformation Provided by Kazanorg.. |
|||
Density | 0.850 - 1.00 g/cc @Temperature 20.0 °C |
0.0307 - 0.0361 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez Pyrolysis Heavy Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis. Application: Used in the production of technical carbon, coak, and dark polymeric petroleum resin.Informa.. |
|||
Density | 0.250 - 1.00 g/cc | 0.00903 - 0.0361 lb/in³ | available range |
MarkeTech Carbon Nanofoam Electrically conductive carbon nanofoams possess many of the properties of traditional aerogel material. These materials are available in the form of monoliths, granules, powders and papers. They ar.. |
|||
Density | 0.7787 - 1.00 g/cc | 0.02813 - 0.0362 lb/in³ | |
Saint-Gobain Chemfab® SlipGrip™ 10 PTFE/Silicone Coated Fiberglass Fabric Description: SlipGrip™ products are PTFE-coated fiberglass fabrics with silicone rubber on one face. This unique combination provides a "slippery" PTFE surface and a "grippy" silicone surface. .. |
|||
Density | 0.980 - 1.00 g/cc | 0.0354 - 0.0361 lb/in³ | |
Wacker Silicones Geniomer® 140 Silicone TPE SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |
|||
Density | 0.980 - 1.00 g/cc | 0.0354 - 0.0361 lb/in³ | |
Wacker Silicones Geniomer® 200 Silicone TPE Elastomer SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |
|||
Density | 0.922 - 1.00 g/cc | 0.0333 - 0.0361 lb/in³ | Spec; ISO 1183-1 |
Axion Polymers Axpoly® PP06 5001 Enhanced Black General Purpose Polypropylene PP06 Series polypropylene offer the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PP06 range of resin co.. |
|||
Density | 0.900 - 1.00 g/cc | 0.0325 - 0.0361 lb/in³ | Free Density |
C.O.I.M. UREXTER® T 404 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Density | 0.980 - 1.00 g/cc | 0.0354 - 0.0361 lb/in³ | |
Wacker Silicones Geniomer® 80 Silicone TPE SLM TPSE 80 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |
|||
Density | 0.917 - 1.00 g/cc | 0.0331 - 0.0361 lb/in³ | Average value: 0.923 g/cc Grade Count:324 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |
|||
Density | 0.980 - 1.00 g/cc | 0.0354 - 0.0361 lb/in³ | |
Wacker Silicones Geniomer® 60 Silicone TPE SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |