Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Mytex Polymers AS88L-01 Polypropylene, Compounded, Elastomer
Description: AS88L-01 is a compounded, elastomer modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications ..
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Polyplastic Armlen® PP GF 20-1EX Polypropylene Copolymer, 20% Glass Fiber
Information provided by PolyPlastic Group.
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Polykemi AB POLYfill PPC TS20020 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Density 1.04 g/cc
0.0376 lb/in³
ASTM Data
Americas Styrenics Styron® XL-8023VC High Impact Polystyrene  (discontinued **)
STYRON® XL-8023 VC high impact polystyrene is designed to provide molders of VCR cassettes with the impact and gloss they require, at economics and processability highly advantaged over ABS resins...
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Polimeri Europa Edistir RCL 600 Polystyrene  (discontinued **)
Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets..
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Ineos Nova 1511 High Heat Crystal Polystyrene  (discontinued **)
High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical..
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Ineos Nova 2110 General Purpose Crystal Polystyrene  (discontinued **)
Moderately high heat resistance, Good balance of strength and ease of processing, USP Class VIApplications: Foam extrusion, Biaxially oriented sheet, Thermoformed drinkware, Molded packagingExposure..
Density 1.04 g/cc
0.0376 lb/in³
DIN 53479
Ineos Nova S-3400 Medium Impact Compact Polystyrene  (discontinued **)
Impact polystyrene with good flow characteristics and a high elongation. Generally used for applications where a tough material is required. For injection molding generally a lubricated type is us..
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Ineos Nova 765 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
High flow, High impact, Color stable, Custom colorsApplications: High flow, multi-purpose injection molding grade where color stability is a requirement, Toys, Appliance, Computer peripheralsPerform..
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Ineos Nova 5404 High Impact Polystyrene
High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were..
Density 1.04 g/cc
0.0376 lb/in³
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA)
High-impact grade of polystyrene with improved impact strength and heat resistance, developed for injection molding and extrusion/thermoforming applications.Information provided by BASF.Ineos Styren..
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Inno-Comp INNOPOL® CS 1-7120 AP 20% Talc Filled Polypropylene Homopolymer
INNOPOL® CS 1-7120 is a 20 % talc-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-7120 is recommended for extrusion of sheet..
Density 1.04 g/cc
0.0376 lb/in³
Momentive Performance Materials RTV6809 Aluminum Adhesive Sealant, Industrial Plastic Adhesive
One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: Primerless adhesion to many ..
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
LG Chemical 60HR-G HIPS
High flow, Heat resistance, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include TV sets, tape reco..
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183/A
Solvay TECHNYL® eXten D 458P PA6.10, DRY
Description: Product in development - provisional datasheet. High viscosity unfilled plasticized PA6.10 for extrusion applications providing low end part warpage.Available in: Asia Pacific, Europe, ..
Density 1.04 g/cc
0.0376 lb/in³
ASTM D 792
Styrolution PS 6210/6211 HIPS
Great balance of rigidity and toughnessUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution
Density 1.04 g/cc
0.0376 lb/in³
ASTM Data
Styron Magnumâ„¢ 555 ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Density 1.04 g/cc
0.0376 lb/in³
ASTM Data
Styron Magnumâ„¢ 941 ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Density 1.04 - 1.06 g/cc
0.0376 - 0.0383 lb/in³
RP-0064
Solvay ALKAMULS® EL 620LI Surfactant
Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 12.Chemical Name: CASTOR OIL ETHOXYLATE(30)CAS: 61791-12-6, 7732-18-5A..
Density 1.04 g/cc

@Temperature 50.0 °C
0.0376 lb/in³

@Temperature 122 °F
Solvay ALKAMULS® OR 36 Surfactant
Description: Ethoxylated castor oil. Emulsifier for oil and waxes in water based formulations. Used as dispersant for pigments and iron powders. Dispersant for pigments and iron powders in magnetic ..
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP MF004S PP
LNP THERMOCOMP* MF004S is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized.
Density 1.04 - 1.07 g/cc
0.0376 - 0.0387 lb/in³
Trelleborg Emerson & Cuming Eccobond® 45C Two-Component General Purpose Epoxy Adhesive
Emerson & Cuming 45C Eccobond® Two-Component General Purpose Epoxy AdhesiveClear, unfilled, general purpose, room temperature curing, epoxy adhesive and sealant. Flexibility can be adjusted by the ..
Density 1.04 g/cc
0.0376 lb/in³
Arkema Group Orgalloy® LE 60SF Flexible Nylon Alloy (Conditioned)
LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).lower in viscosity than LE 6000, adapted to Suited to the cast film..
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Aclo Accutech Polypropylene Homopolymer HP0336T20L Talc Reinforced
Density 1.04 g/cc
0.0376 lb/in³
BASF Procom® D 1085 Polypropylene
Data was collected by ISO methods and provided by BASF.
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Beijing Chemical Industry KAIFA® GL6000 ABS Metal Plating Grade
Excellent plating performance, Good thermal stabilityInformation provided by Beijing Chemical Industry Research Institute (Group)
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Adell EQ-14 Homopolymer Polypropylene, 20% Mica Filled
Data provided by Adell Plastics, Inc.
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Ineos Nova 1220 High Heat Crystal Polystyrene  (discontinued **)
Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r..
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
EMS-Grivory Grivory® TR 55 LY PA12/MACMI
Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LY offers a variety of interesting properties such as: c..