Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.44 g/cc | 0.0520 lb/in³ | (Dry) |
BASF Capron® GR40 HS 40% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR40 HS is a heat stabilized 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stabil.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO data |
BASF Capron® GR40 HS 40% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR40 HS is a heat stabilized 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stabil.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183/B |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
LATI LATILUB 73/13-01M Polyoxymethylene Base (POM), 1% Molybdenum Disulfide Self Lubricating Plastic
(Unv Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
Kleerdex Kydex® IM90 Acrylic/PVC injection Molding Compound
(discontinued **) Low heat release aviation gradeApplications: Kydex IM90 is designed for injection molded parts each need to meet the highest flammability requirements of the FAA (FAR 25.853d) for vertical burn, rat.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | |
LATI Latilub 73/13-01M POM, Molybdenum disulphide Filled Self-lubricating product based on Polyoxymethylene (POM). Molybdenum disulphide. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati In.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WL004 is a compound based on Polybutylene Terephalate resin containing PTFE. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® ABS GF30 FR 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON OEL32 PPS - Linear LNP* STAT-KON* OCL32 is a compound based on PPS - Linear resin containing 10% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
Techmer ES HiFill® POM CO GF5 CC 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 5% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
Stir SpA RTC PM A (PVC) Application: Shock resistant moldingInformation provided by STIR SpA |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP DF006 PC (Asia Pacific) LNP* Thermocomp* DF006 is a compound based on Polycarbonate resin containing Glass Fiber. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP EC008 PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* EC008 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features include: Electrically Conductive. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP UX06032 PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UX06032 is a compound based on Polyphthalamide resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Non-Brominated & Non-Chlorin.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON OE006A PPS - Branched LNP STAT-KON* OE006A is a compound based on PPS - Branched resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183-87 |
Wellman EcoLon® 2000-BK1 37% Post Consumer Compound Nylon 66 Description: Post Consumer Compound Nylon 66Information provided by Wellman. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | DIN 53479 |
Polyram RamTal PM1609 Acetal, Molybdenum Disulfide Filled Molybdenum disulfide filled polyacetal for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | |
Covestro Makrolon® 8035 Polycarbonate High viscosity extrusion and injection molding grade with 30% short glass fibers and easy mold release, low anisotropy, for stiff moldings requiring good dimensional stability.Information provided b.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® LW9030 BK851 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 BK851 is a 30% glass fiber reinforced black polybutylene terephthalate blend for injection mol.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SC193 NC010 PBT+SAN
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend Developed for the Healthcare IndustryCrastin® SC193 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. It.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
Ensinger Tecapeek® XP-98HT Compression Molded PEEK HT, 30% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
Eurostar Star L PA66 30V D61 PA66, Glass Fiber Filled, Injection Molded Star L PA66 30V D31 is a PTFE/Silicone Lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
Eurotec® Tecopet® PT70 GR15 NL100 PR PET, 15% glass fiber reinforced, heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
Chem Polymer Chemlon 256 Nylon 6, Wire Jacketing Grade A non-halogenated, Allwires rated wire coating grade used primarily on cables for power and control circuits in commercial and industrial applications. The cables are oil, gasoline, and abrasion re.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | JIS-Z-8807 |
Denka VINYKON M2024 PVC, M grade for hard injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® XT-1169 Two-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® HT1V-3 HY black 9205 PA6T/6I-GF30 Product description: Grivory HT1V-3 HY black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-3 HY bl.. |
|||
Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp DFZ42P PC (Asia Pacific) LNP* Thermocomp* DFZ42P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the.. |