Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.37 - 1.54 g/cc | 0.0495 - 0.0556 lb/in³ | Average value: 1.48 g/cc Grade Count:5 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i.. |
|||
Density | 1.08 - 1.54 g/cc | 0.0390 - 0.0556 lb/in³ | Average value: 1.30 g/cc Grade Count:65 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Density | 0.962 - 1.54 g/cc | 0.0348 - 0.0555 lb/in³ | Average value: 1.29 g/cc Grade Count:107 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Density | 1.36 - 1.54 g/cc | 0.0491 - 0.0556 lb/in³ | Average value: 1.43 g/cc Grade Count:10 |
Overview of materials for Phenolic, Resole, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Wood Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Density | 1.39 - 1.54 g/cc | 0.0502 - 0.0556 lb/in³ | Average value: 1.44 g/cc Grade Count:22 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Density | 1.18 - 1.54 g/cc | 0.0426 - 0.0556 lb/in³ | Average value: 1.32 g/cc Grade Count:86 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Density | 1.21 - 1.54 g/cc | 0.0437 - 0.0556 lb/in³ | Average value: 1.35 g/cc Grade Count:20 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 412 Rigid PVC, Extrusion Electric channels |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 412/L Rigid PVC, Extrusion Corrugated plastics |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 620 Rigid PVC, Extrusion Spiral pipes |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | ISO R 1184 |
Fainplast Compounds RKS 325/W-UV Rigid PVC, Antishock Extrusion Lead Free Various profiles, antishock UV resistant |
|||
Density | 1.40 - 1.54 g/cc | 0.0506 - 0.0556 lb/in³ | 310A Resin |
Lord Adhesives Fusor® 310 A/B Epoxy Adhesive Lord® 310 adhesive is a modified, thixotropic, two-part epoxy adhesive which bonds well to many types of prepared metals, prepared rubber, urethane, and plastics. Originally formulated for primer.. |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | ISO R 1183 |
Fainplast Compounds AP 75 Flexible PVC, Flame Retardant Insulation General purposes |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | ISO R 1183 |
Fainplast Compounds AP 87/1 Flexible PVC, Flame Retardant Insulation General purposes |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 86/6 Flexible PVC, Sheathing General purposes |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 88 Flexible PVC, Insulation General purposes |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 89 Flexible PVC, Insulation General purposes |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 80/2 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 89/2 Flexible PVC, Flame Retardant Sheathing Lead Free Special cables |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 91 Flexible PVC, Flame Retardant Sheathing Lead Free Operating temperature 80°C |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 018/27F Halogen Free PVC Sheathing, designed to meet VDE 0207 part 24 HM4 |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 045 Halogen Free PVC General purpose; improved fire performance |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 38 Halogen Free PVC General purpose |
|||
Density | 1.52 - 1.54 g/cc | 0.0549 - 0.0556 lb/in³ | ASTM D792 |
Chang Chun Plastic PBT3030 30% Glass Fiber Enforced PBT Information provided by Dowell Trading Company Ltd. |
|||
Density | 1.44 - 1.54 g/cc | 0.0520 - 0.0556 lb/in³ | Average value: 1.51 g/cc Grade Count:39 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 32 Halogen Free PVC General purpose |
|||
Density | 1.50 - 1.54 g/cc | 0.0542 - 0.0556 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 76/E Flexible PVC, Sheathing General purposes |