Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.66 g/cc | 0.0600 lb/in³ | STN 64 0111 |
Plastcom SLOVASTER® B GF 30 FRK 3 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Polystrand ThermoPro™ IE7010X X-Ply Cross-Ply Polypropylene-Glass Composite 2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Polystrand ThermoPro™ IE7020X X-Ply Cross-Ply Polyethylene-Glass Composite 2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Polystrand ThermoPro™ IS7015X X-Ply Cross-Ply Polypropylene-Glass Composite 2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous S-Glass (ThermoPro-S™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK608 BK509 PBT
(Unverified Data**) Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
DSM Akulon® K-FHG12 (Dry) 60% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Density | 1.66 - 1.92 g/cc | 0.0600 - 0.0694 lb/in³ | Average value: 1.77 g/cc Grade Count:15 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
Lanxess Pocan® DP BF 4232 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183/A |
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, Conditioned Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, heat and UV stabilized, characterized by a high fluidity of the melt, for injection molding.Available in: Europe Product Applic.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® VX8532 PBT+PET (Europe-Africa-Middle East) VALOX VX8532 is a 30% glassfiber reinforced, non blooming, flame retardant PBT+PET blend with excellent surface appearance and good ultrasonic weldability properties.This data was supplied by SABIC-.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | GB/T 1033.1-2008 |
Sichuan Deyang Haton® hGR302 PPS / F4 Polyphenylene Sulfide Injection molding, anti-frictionInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP OCF62E PPS - Branched LNP* THERMOCOMP* OCF62E is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp WB008 PBT LNP* Thermocomp* WB008 is a compound based on Thermoplastic Polyester (PBT) containing Glass Beads.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON UV00ASU PPA LNP* VERTON* UV00ASU is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: UV Stabilized, Heat Stabilized, Structural. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
Unitika RUN35-C25 PA6, Conditioned High modulus and low warpage nylonInformation provided by Unitika Ltd. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
Unitika RUN35-C25 PA6, Dry High modulus and low warpage nylonInformation provided by Unitika Ltd. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D792 |
Unitika RUN35-C25 Weather resistant PA6, Dry Weather resistant, noncoating, external exposure-compatibleInformation provided by Unitika Ltd. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
DSM Akulon® Ultraflow™ K-FHG12 Nylon 6-60% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)
(Unverified Data**) 45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |
|||
Density | 1.66 - 1.86 g/cc | 0.0600 - 0.0672 lb/in³ | Average value: 1.77 g/cc Grade Count:12 |
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | Liquid |
3M Novec™ 7300 Engineered Fluid 3M™ Novec™ 7300 fluid is a clear, colorless, odorless fluid that has utility in a wide variety of applications, including heat transfer, lubricant deposition, electronic testing and cleaning appli.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | Liquid |
3M Novec™ 7300DL Engineered Fluid 3M™ Novec™ 7300DL fluid is a clear, colorless, odorless fluid. A high-purity version of 3M™ Novec™ 7300 fluid, designed for demanding applications such as hard disk lubricant deposition & semico.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D792 |
Unitika RUN35-C25 Weather resistant PA6, Conditioned Weather resistant, noncoating, external exposure-compatibleInformation provided by Unitika Ltd. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
Vyncolit Neopreg Kinel® SK4525 S5 Glass Fiber Reinforced Molding Compound BMI molding compound long glass fiber reinforced with excellent mechanical and thermal properties. Especially suited to be used for injection molding.Information provided by Sumitomo Bak North Ameri.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PBT 0166 B FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |