Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
Multibase Multi-Pro® 7518 C Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
Plenco 51045 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is It is UL listed and available in black only.Information supplied b.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | |
Haveg 41NA Phenolic; Silicate Filled A proprietary thermoset plastic consisting of a phenol-formaldehyde resin and non-asbestos silicate fillers. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO R 1183 |
Multibase Multibatch® MP 50009 Anti-split CPP. 70% CaCO3 Filled.Carpet Backing.Information provided by Multibase |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | |
LATI Latilub 80-10T G/40 PPS, 40% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP PF00C PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PF00C is a compound based on PA6 resin containing Glass Fiber. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp RF00CS PA 66 LNP* Thermocomp* RF00CS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXS PA 66 (Asia Pacific) LNP* Thermocomp* RF00CSXS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXS PA 66 (Asia Pacific) LNP* Thermocomp* RF00CSXS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP PF00CS PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PF00CS is a compound based on PA6 resin containing Glass Fiber. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXZ PA 66 LNP* THERMOCOMP* RF00CSXZ is a compound based on Recycled Nylon 66 resin containing 60% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
Solvay TECHNYL® 2912GMH7-P PA66, 63% glass fiber, DRY Description: Polyamide 66, reinforced with 63% of glass fiber for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2912GMH7-P is used in all sectors of industry, offerin.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | |
Cosmic Plastics D69 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60 Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK609 NC010 PBT
(Unverified Data**) Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)
(Unverified Data**) 60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo.. |
|||
Density | 1.72 g/cc @Temperature 23.0 °C |
0.0621 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Density | 1.72 - 1.94 g/cc | 0.0620 - 0.0700 lb/in³ | ASTM D792 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Density | 1.72 - 1.94 g/cc | 0.0620 - 0.0700 lb/in³ | ASTM D792 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Density | 1.72 - 1.94 g/cc | 0.0620 - 0.0700 lb/in³ | ASTM D792 |
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Density | 1.72 - 1.94 g/cc | 0.0620 - 0.0700 lb/in³ | ASTM D792 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Density | 1.72 g/cc @Temperature 40.0 °C |
0.0621 lb/in³ @Temperature 104 °F |
Liquid |
3M Novec™ 774 Engineered Fluid 3M™ Novec™ 774 Engineered Fluid is a clear, colorless and low odor fluid, and is one in a line of 3M products designed as replacements for ozone depleting substances (ODSs) and compounds with high.. |
|||
Density | 1.72 - 1.92 g/cc | 0.0621 - 0.0694 lb/in³ | Molded |
Bulk Molding Compounds BMC T40(18)V0 Die Casting Replacement Grade Molding Compound BMC T40(18)V0 is a lower cost version of BMC T40(18) where a UL 5V rating is not necessary. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled
(discontinued **) LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat.. |
|||
Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled
(discontinued **) LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat.. |